期刊文献+

Researches on the PAM/Cr^3+ Gel for Deep Profile Control 被引量:1

一种用于深部调堵的PAM/Cr^(3+)凝胶的研究(英文)
下载PDF
导出
摘要 The profile control hard-gel is composed of polyarylamide (5-6g/L), whose molecular weight is 4,000,000 - 7,000,000 and hydrolysis degree is 17.6%, and cross-linking oxidation-reduction agent (Na2Cr2O7 + NH4Cl), with an delayed organic acid crosslinker which contains lactic acid/propionic acid/ethanoic acid and ethylene glycol. After research of the influence factors, such as pH, temperature, salinity and the dosage of delayed crosslinker, the optimum condition(pH 5.2, temperature 55℃, salinity < 7g/L) was found. Gelation time (12-144h) can be controlled by adjusting the dosage of the delayed crosslinker. Deep profile control experiments are carried out on heterogeneous models, which contains three serial high permeable and low permeable cores arranged in a parallel. After water flooding (total recovery, 24.3%), the first, second and third high-permeable cores each are sealed in turn by the profile control agent, and the total displacement recovery increases to 46.8%, 62.2% and 69.1% respectively. So, the greater the sealed depth, the larger the enhancing recovery will be. Finally, the oil displacement mechanisms of deep profile control are discussed. The profile control hard-gel is composed of polyarylamide (5-6g/L), whose molecular weight is 4,000,000 - 7,000,000 and hydrolysis degree is 17.6%, and cross-linking oxidation-reduction agent (Na2Cr2O7 + NH4Cl), with an delayed organic acid crosslinker which contains lactic acid/propionic acid/ethanoic acid and ethylene glycol. After research of the influence factors, such as pH, temperature, salinity and the dosage of delayed crosslinker, the optimum condition(pH 5.2, temperature 55℃, salinity < 7g/L) was found. Gelation time (12-144h) can be controlled by adjusting the dosage of the delayed crosslinker. Deep profile control experiments are carried out on heterogeneous models, which contains three serial high permeable and low permeable cores arranged in a parallel. After water flooding (total recovery, 24.3%), the first, second and third high-permeable cores each are sealed in turn by the profile control agent, and the total displacement recovery increases to 46.8%, 62.2% and 69.1% respectively. So, the greater the sealed depth, the larger the enhancing recovery will be. Finally, the oil displacement mechanisms of deep profile control are discussed.
出处 《Petroleum Science》 SCIE CAS CSCD 2004年第1期65-69,共5页 石油科学(英文版)
关键词 Deep profile control hard-gel delayed cross-linker gelation time heterogeneous model sealed depth Deep profile control, hard-gel, delayed cross-linker, gelation time, heterogeneous model, sealed depth
  • 相关文献

同被引文献16

引证文献1

二级引证文献52

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部