根据分形几何理论的基本概念,就无序分形多孔介质孔隙率φ和渗透率K与多孔介质结构分数维数Df的关系进行了推导,利用Sierpinski固相分形体(Solid mass fractal)与孔相分形体(Pore mass fractal)概念对分形多孔介质微结构特征、孔隙累积...根据分形几何理论的基本概念,就无序分形多孔介质孔隙率φ和渗透率K与多孔介质结构分数维数Df的关系进行了推导,利用Sierpinski固相分形体(Solid mass fractal)与孔相分形体(Pore mass fractal)概念对分形多孔介质微结构特征、孔隙累积数量-尺寸分布和孔隙率φ等参数及其物理关系给予了详细论述,定量地分析和讨论了基于不同模型的渗透率-分形维数关系与它们的差异。展开更多
The effects of phosphorus and boron addition on the as-cast microstructure and homogenization parameters of Inconel 718 were studied. The results indicate that the addition of phosphorus and boron promotes the formati...The effects of phosphorus and boron addition on the as-cast microstructure and homogenization parameters of Inconel 718 were studied. The results indicate that the addition of phosphorus and boron promotes the formation of blocky Laves phase. Due to the strong segregation behavior of boron in the final residual liquid, a low melting B-bearing phase enriched in Nb, Mo and Cr is observed. According to the differential scanning calorimeter results and electron probe micro-analysis characterization, the solidification sequence of Inconel 718 with phosphorus and boron addition in best combination is determined as L→L+γ→L+γ+MC→L+γ+MC+Laves→γ+MC+Laves+MC+Laves+B-bearing phase. Accordingly, the homogenization temperature is recommended to be adjusted at least 40°C lower than that of standard Inconel 718 due to the existence of low melting B-bearing phase.展开更多
文摘根据分形几何理论的基本概念,就无序分形多孔介质孔隙率φ和渗透率K与多孔介质结构分数维数Df的关系进行了推导,利用Sierpinski固相分形体(Solid mass fractal)与孔相分形体(Pore mass fractal)概念对分形多孔介质微结构特征、孔隙累积数量-尺寸分布和孔隙率φ等参数及其物理关系给予了详细论述,定量地分析和讨论了基于不同模型的渗透率-分形维数关系与它们的差异。
基金Project (08dj1400402) supported by the Major Program for the Fundamental Research of Shanghai Committee of Science and Technology,China
文摘The effects of phosphorus and boron addition on the as-cast microstructure and homogenization parameters of Inconel 718 were studied. The results indicate that the addition of phosphorus and boron promotes the formation of blocky Laves phase. Due to the strong segregation behavior of boron in the final residual liquid, a low melting B-bearing phase enriched in Nb, Mo and Cr is observed. According to the differential scanning calorimeter results and electron probe micro-analysis characterization, the solidification sequence of Inconel 718 with phosphorus and boron addition in best combination is determined as L→L+γ→L+γ+MC→L+γ+MC+Laves→γ+MC+Laves+MC+Laves+B-bearing phase. Accordingly, the homogenization temperature is recommended to be adjusted at least 40°C lower than that of standard Inconel 718 due to the existence of low melting B-bearing phase.