采用微乳液法制备出粒径约为80 nm,主要成分为α-Fe的纳米铁粒子。纳米铁具有极高的活性,在无氧环境中,室温、中性条件下与初始质量浓度为30、50、80、120 mg/L的NO3--N振荡反应30 m in,即可获得90%以上的脱硝率。零价纳米铁去除硝酸盐...采用微乳液法制备出粒径约为80 nm,主要成分为α-Fe的纳米铁粒子。纳米铁具有极高的活性,在无氧环境中,室温、中性条件下与初始质量浓度为30、50、80、120 mg/L的NO3--N振荡反应30 m in,即可获得90%以上的脱硝率。零价纳米铁去除硝酸盐氮的一系列批实验结果表明:硝酸盐与纳米铁反应为非一级动力学反应,硝酸盐氮浓度随时间单调减少,氨氮浓度随时间单调升高,而亚硝酸盐氮的浓度在反应过程中出现极大值,由动力学分析可知其具有连续反应的突出特征,并以此对反应路径进行了探讨。提出纳米铁与硝酸盐反应是氧化还原与吸附作用同时存在且主要产物为氨氮的观点。展开更多
Using Ancrocalorimetric method, the thermally measured curves of differenttypes of metabolism of E. coli were detendned. nom these thermal measured cu-rves, wecan obtain the heat output of E. coll at growth metabolism...Using Ancrocalorimetric method, the thermally measured curves of differenttypes of metabolism of E. coli were detendned. nom these thermal measured cu-rves, wecan obtain the heat output of E. coll at growth metabolism to be 1 .74+10.63 pW.cell- 1; and0.14+0.04 pW.cell-1 at the non-growth metabolism while at the endogenous metabolismit is 0.045+0.001 pW.展开更多
文摘采用微乳液法制备出粒径约为80 nm,主要成分为α-Fe的纳米铁粒子。纳米铁具有极高的活性,在无氧环境中,室温、中性条件下与初始质量浓度为30、50、80、120 mg/L的NO3--N振荡反应30 m in,即可获得90%以上的脱硝率。零价纳米铁去除硝酸盐氮的一系列批实验结果表明:硝酸盐与纳米铁反应为非一级动力学反应,硝酸盐氮浓度随时间单调减少,氨氮浓度随时间单调升高,而亚硝酸盐氮的浓度在反应过程中出现极大值,由动力学分析可知其具有连续反应的突出特征,并以此对反应路径进行了探讨。提出纳米铁与硝酸盐反应是氧化还原与吸附作用同时存在且主要产物为氨氮的观点。
文摘Using Ancrocalorimetric method, the thermally measured curves of differenttypes of metabolism of E. coli were detendned. nom these thermal measured cu-rves, wecan obtain the heat output of E. coll at growth metabolism to be 1 .74+10.63 pW.cell- 1; and0.14+0.04 pW.cell-1 at the non-growth metabolism while at the endogenous metabolismit is 0.045+0.001 pW.