Enhanced recovery of zinc and lead by slag composition optimization in rotary kiln 被引量:3
1
作者 hong-fu lin Wei WENG +1 位作者 Shui-ping ZHONG Guan-zhou QIU 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第9期3110-3122,共13页
High-efficiency recovery of Zn and Pb from silicon-rich zinc leaching residues is realized in a rotary kiln.Characterizations by means of XRD,SEM,EDS and ICP reveal that the leaching residue contains 12.4 wt.%SiO_(2),... High-efficiency recovery of Zn and Pb from silicon-rich zinc leaching residues is realized in a rotary kiln.Characterizations by means of XRD,SEM,EDS and ICP reveal that the leaching residue contains 12.4 wt.%SiO_(2),16.1 wt.%Zn,and 7.4 wt.%Pb.Thermodynamic analysis shows that metallic vapor of Zn and Pb can be easily generated from the zinc leaching residue at 1150-1250°C inside the rotary kiln.Viscosities and melting points of 13 slag compositions were analyzed and three slag compositions(47wt.%SiO_(2)-23wt.%CaO-30wt.%FeO,40wt.%SiO_(2)-28wt.%CaO-32wt.%FeO,and 40wt.%SiO_(2)-30wt.%CaO-30wt.%FeO)possessed the desirable physical properties,with the melting point and viscosity in the range of 1150-1280°C and 0.2-0.5 Pa·s,respectively.The industrial tests show that adopting the optimized slag composition can contribute to very high recovery rates of Zn and Pb(97.3%for Zn and 94.5%for Pb),corresponding to slags with very low average contents of Zn and Pb(0.51 wt.%Zn and 0.45 wt.%Pb).The National-Standard leaching tests of the water-quenched slags result in 1.82 mg/L Zn,~0.01 mg/L Cu,0.0004 mg/L As,~0.01 mg/L Cd,0.08 mg/L Pb,and~0.02 mg/L Hg in the leachate,verifying the detoxification of the zinc leaching residue at the same time. 展开更多
关键词 zinc leaching residues metals recovery rotary kiln slag composition optimization DETOXIFICATION
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部