The effect of different decomposition conditions on tungsten recovery forscheelite concentrate has been examined. The results show that tungsten recovery can be more than98% under decomposing conditions as follows: th...The effect of different decomposition conditions on tungsten recovery forscheelite concentrate has been examined. The results show that tungsten recovery can be more than98% under decomposing conditions as follows: the amount of caustic soda is 2.2 and 3.2 times oftheoretical respectively, ratio of water and ore is 0.7-0.8, temperature is 160℃, and preservationtime is 2.0 h for scheelite concentrate (63.21 % WO_3) and low grade scheelite concentrate (55.17%WO_3).展开更多
文摘The effect of different decomposition conditions on tungsten recovery forscheelite concentrate has been examined. The results show that tungsten recovery can be more than98% under decomposing conditions as follows: the amount of caustic soda is 2.2 and 3.2 times oftheoretical respectively, ratio of water and ore is 0.7-0.8, temperature is 160℃, and preservationtime is 2.0 h for scheelite concentrate (63.21 % WO_3) and low grade scheelite concentrate (55.17%WO_3).