Effects of welding parameters and post-heat treatment on mechanical properties of friction stir welded AA2195-T8 Al-Li alloy 被引量:17
1
作者 J. Zhang X.S. Feng +3 位作者 J.S. Gao H. Huang Z.Q. Ma L.J. Guo 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2018年第1期219-227,共9页
In this study, the effects of main welding parameters (rotation speed (ω) and welding speed (υ)) on the microstructure, micro-hardness distribution and tensile properties of friction stir welded (FSW) 2195-T... In this study, the effects of main welding parameters (rotation speed (ω) and welding speed (υ)) on the microstructure, micro-hardness distribution and tensile properties of friction stir welded (FSW) 2195-T8 Al-Li alloy were investigated. The effects of T6 post-treatments at different solution and aging conditions on the mechanical properties and microstructure characteristics of the FSW joints were also investigated. The results show that with increasing to and v, both strength and elongation of the joints increase first, and then decrease with further increase of ω and υ. All the joints under varied welding parameters show significant strength loss, and the strength reaches only 65% of the base metal, The effect of T6 post-heat treatment on the mechanical properties of the joints depends on the solution and aging conditions. Two heat treatment processes (480 ℃×0.5 h quenching+ 180 ℃× 12 h, 520 ℃× 0.5 h quenching+ 180 ℃×12h aging) are found to increase the joint strength. Furthermore, low temperature quenching (480℃) is more beneficial to the joint strength. The joint strength can reach 85% of the base metal. Whereas both low temperature aging (140 ℃× 56h) and stepped aging ( 100 ℃× 12 h + 180 ℃× 3 h) processes decrease the joint strength. After heat treatment all the joints show decreased ductility due to the obvious grain coarsening in the nugget zone (NZ) and thermo-mechanically affected zone (TMAZ). 展开更多
关键词 2195-t8 Al-Li alloy Friction stir welding Welding parameters Post-heat treatment
原文传递
拉-拉载荷下2195-T8铝锂合金在N_(2)O_(4)中的预腐蚀疲劳研究 被引量:1
2
作者 郭一 常新龙 +3 位作者 田干 刘德俊 庞闯 吴畏 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2022年第9期3459-3465,共7页
液体导弹在长期加注贮存的状态下,弹体与贮箱结构常因腐蚀损伤从而导致疲劳裂纹的产生乃至断裂等问题。采用疲劳寿命测试、扫描电镜以及能谱分析等方法,研究了2195-T8铝锂合金在N_(2)O_(4)中预腐蚀180d后的疲劳裂纹萌生、扩展和断裂机制... 液体导弹在长期加注贮存的状态下,弹体与贮箱结构常因腐蚀损伤从而导致疲劳裂纹的产生乃至断裂等问题。采用疲劳寿命测试、扫描电镜以及能谱分析等方法,研究了2195-T8铝锂合金在N_(2)O_(4)中预腐蚀180d后的疲劳裂纹萌生、扩展和断裂机制,并与未腐蚀试样进行对比。结果表明:2种环境下试样的疲劳极限为145、118MPa,循环应力降低比值约为18.62%;试样在预腐蚀的过程中,由于形成“闭塞区”,同时与富铜相粒子形成原电池,进一步加速腐蚀历程,形成多源裂纹萌生的特征,且更易从非金属夹杂区域起裂;受到晶粒间的位错、堆积等因素的影响,发现了垂直于疲劳辉纹、穿越大晶粒及途经小角度晶界的二次裂纹;2种环境中的疲劳瞬断区的断口形貌呈现出典型的沿晶韧窝和韧性断裂的特征。 展开更多
关键词 2195-t8铝锂合金 预腐蚀损伤 疲劳寿命 断口分析 二次裂纹
原文传递
NaCl溶液中Al-Li合金腐蚀过程的电化学特征 被引量:16
3
作者 李劲风 张 昭 +4 位作者 程英亮 曹发和 王建明 张鉴清 曹楚南 《金属学报》 SCIE EI CAS CSCD 北大核心 2002年第7期760-764,共5页
采用电化学噪声技术,结合电化学阻抗谱及极化曲线测量,研究了峰时效AA2195-T8铝合金在3.0%NaCl溶液中的腐蚀电化学特征.结果表明,腐蚀初期,合金表面钝化膜上不断有孔核的形成与修复,并导致阻抗谱上感抗成分的存在.随腐蚀时间的延长,其... 采用电化学噪声技术,结合电化学阻抗谱及极化曲线测量,研究了峰时效AA2195-T8铝合金在3.0%NaCl溶液中的腐蚀电化学特征.结果表明,腐蚀初期,合金表面钝化膜上不断有孔核的形成与修复,并导致阻抗谱上感抗成分的存在.随腐蚀时间的延长,其感抗成分消失且阻抗模值降低.阳极极化时,由于其孔蚀电位与自腐蚀电位接近,钝化电位区间很小;随腐蚀时间的延长,极化电阻先增加而后减小,自腐蚀电流则呈相反趋势变化. 展开更多
关键词 AA2195-t8铝合金 NACL溶液 腐蚀 电化学噪声 阻抗谱 极化曲线