Development and Application of High-Performance Magnesia-Chrome Bricks for RH Degasser
1
作者 ZHAO Huimin , BI Yubao , LIU Xiongzhang and CHU Xuetian(Luoyang Refractory (Group) Co. , Henan, 471039, China) 《China's Refractories》 CAS 2002年第4期25-29,共5页
The paper analyses the wear mechanism of magnesia-chrome bricks for snorkel of RH degasser. High-performance magnesia-chrome bricks with good resistance to molten slag and infiltration resistance have been manufacture... The paper analyses the wear mechanism of magnesia-chrome bricks for snorkel of RH degasser. High-performance magnesia-chrome bricks with good resistance to molten slag and infiltration resistance have been manufactured by means of reasonable fabricating technology. The application results of the developed magnesia-chrome bricks at 300t RH degasser of Baosteel indicate that the lining life has been increased up to 150 heats. 展开更多
关键词 SNORKEL magnesia-chrome brick WEAR Infiltration resistance Secondary metallurgy
下载PDF
The State-of-art of Magnesia-chrome Refractories for P-S Converter in China's Non-ferrous Industry
2
作者 CHENKaixian LIYong 《China's Refractories》 CAS 2002年第2期18-21,共4页
The state-of-art of magnesia-chrome refractories from direct-bonded magnesia chrome brick to fused-grain rebounded magnesia chrome brick for P-S converter is dis-cribed. The Cr2O3 content of the brick is continually i... The state-of-art of magnesia-chrome refractories from direct-bonded magnesia chrome brick to fused-grain rebounded magnesia chrome brick for P-S converter is dis-cribed. The Cr2O3 content of the brick is continually increased with the reduction of the impurity content of brick , the pre-synthetic raw material it applied and the operating condition of convener is optimized so that the service life of convener is largely enhanced. 展开更多
关键词 magnesia-chrome brick Development CONVERTER Non-ferrous industry
下载PDF
Effect of Magnesia-Chrome Synthetic Materials on Magnesia-Alumina-Chrome Ramming Mixes
3
作者 WANG Li ZHANG Xiaohui +1 位作者 ZHANG Chenqian JIANG Mingxue 《China's Refractories》 CAS 2006年第3期24-27,共4页
Magnesia-alumina-chrome ramming mixes with same chemical compositions were prepared by using different raw materials such as fused magnesia-chrome synthetic materials and sintered one, wasted bricks and magnesia-alumi... Magnesia-alumina-chrome ramming mixes with same chemical compositions were prepared by using different raw materials such as fused magnesia-chrome synthetic materials and sintered one, wasted bricks and magnesia-alumina spinels. Their physical properties were tested and microstructures were analyzed. The results show that the ramming mixes made of different raw materials bring about different microstructures and properties although the mixes have the same chemical composition, binder content and aggregate size composition. 展开更多
关键词 magnesia-chrome synthetic materials Ramming mix Magnesia-alumina-chrome
下载PDF
Magnesia-Chrome Refractories for Flash Furnace
4
作者 LI Yong, CHEN Kaixian, LU Xinghua, LIU Jianlong, SUN Jialin , HONG Yanruo (Luoyang Refractories Group Co. , Ltd 471039 P. R. China) University of Science and Technology Beijing, Beijing 100083,China 《China's Refractories》 CAS 2002年第1期9-12,共4页
The rapid development of our country' s heavy non-ferrous metallurgical technology and the revolution in new type of heavynon-ferrous metallurgical furnace have imposed more critical demand on the refractory mater... The rapid development of our country' s heavy non-ferrous metallurgical technology and the revolution in new type of heavynon-ferrous metallurgical furnace have imposed more critical demand on the refractory materials ,i.e. high quality and long service life. This paper presents the domestic status of the refractories for flash furnace , briefly describes the wear of the refractory used, andit is considered that the domestic in refractories for flash-furnace can be surely realized. 展开更多
关键词 Flash furnace magnesia-chrome refractories WEAR
下载PDF
Magnesia,Magnesia-alumina and Magnesia-chrome Refractory Mortars
5
作者 Zhang Xiaohui 《China's Refractories》 CAS 2012年第4期40-42,共3页
This standard specifies the classification, technical requirements, test methods, quality appraisal procedures, packing, marking, transportation, storage, and quality certificate of magnesia, magnesia - alumina and ma... This standard specifies the classification, technical requirements, test methods, quality appraisal procedures, packing, marking, transportation, storage, and quality certificate of magnesia, magnesia - alumina and magnesiachrome refractory mortars. 展开更多
关键词 GB Magnesia Magnesia-alumina and magnesia-chrome Refractory Mortars MN
下载PDF
Sintering Complexity of Magnesia-chrome Refractories
6
作者 GUO Zongqi MA Ying LI Yong 《China's Refractories》 CAS 2022年第1期16-23,共8页
Magnesia-chrome refractories are appropriate to work under cyclic temperatures or atmospheric conditions because some oxides of chrome ore readily release oxygen(are reduced)upon heating and pick up oxygen(are oxidize... Magnesia-chrome refractories are appropriate to work under cyclic temperatures or atmospheric conditions because some oxides of chrome ore readily release oxygen(are reduced)upon heating and pick up oxygen(are oxidized)upon cooling or upon changing the atmosphere.They have been ideal lining materials for RH degassers for many years,despite challenging of Cr^(6+) disposal issue after using.The varieties of magnesia-chrome refractories depend on their raw materials and burning temperatures,which could be well demonstrated by their microstructures.But Indian chrome concentrate cannot be directly used in the production of magnesia-chrome bricks because of reducing sintering density.Silicate bonded magnesia-chrome bricks are produced with low purity magnesia after burning at relatively lower temperatures,resulting in liquid film forming as silicate bond around chrome ore particles.Direct bonded and rebonded fused-grains magnesia-chrome refractories are made of high purity magnesia or fused magnesia-chrome grains,forming euhedral and intergranular secondary chromite spinels as the main feature.The amount of secondary spinel increases with the rising burning temperature,leading to increasing hot modulus of rupture and overall hot properties as well.It is important to burn magnesia-chrome bricks under weakly reducing atmosphere.The oxygen content of burning atmosphere from 800℃ to 1650℃ would better controlled below 0.5%to increase the burnt strength and to avoid inner cracks and loose bonding of magnesia-chrome bricks,while the atmosphere contains 3%-6%O_(2) under most economical firing condition. 展开更多
关键词 magnesia-chrome refractory silicate bond direct bond secondary chromite spinel
下载PDF
Magnesia-Chrome Brick
7
作者 ZHANG Xiaohui 《China's Refractories》 CAS 2007年第4期33-35,共3页
This standard specifies the classification, technical requirements, test method, quality examination regulation, packing, transportation and storage of magnesia-chrome brick.
关键词 magnesia-chrome Brick MPA
下载PDF
Corrosion of Magnesia-chrome Brick by Smelting Reduction Slag with Iron Bath
8
作者 LI Jianqiang WANG Wenwu +1 位作者 GAN Feifang WU Jiguang 《China's Refractories》 CAS 2013年第3期32-37,共6页
Effects of FeO content (0, 5%, 10%, and 15% in mass, respectively ) in lab-synthesized smelting redttc- tion slag with iron bath and test temperature (1 450, 1 500, 1550, anti 1 600 ℃ ) on corrosion am,amount and... Effects of FeO content (0, 5%, 10%, and 15% in mass, respectively ) in lab-synthesized smelting redttc- tion slag with iron bath and test temperature (1 450, 1 500, 1550, anti 1 600 ℃ ) on corrosion am,amount and microstructure of fused rebonded magnesia - chrome brick with 26.02 massqc of Cr2O3 were researched by rotary cylinder method. The results show that : ( 1 ) the corro- sion amolult of magnesia -chrome brick by slag without FeO is higher than that by the slag with 5% FeO, and the vorrosion amount increases when FeO content increa- ses from 5% to 15% ; (2) the test temperature is one of the important factors affecting the slag corrosion resist- ance of magnesia - chrome brick, and the corrosion of smelting reduction slag to brick increases with the temperature rising. 展开更多
关键词 smelting reduction slag with iron bath magnesia - chrome brick CORROSION
下载PDF
铜冶炼侧吹炉用镁铬质耐火材料损毁机制 被引量:1
9
作者 付琪琪 钟立桦 +2 位作者 白文献 淦永彤 邓俊杰 《耐火材料》 CAS 北大核心 2024年第2期148-154,共7页
为了保证新工艺下侧吹炉的安全稳定运行,采用扫描电子显微镜、能谱仪分析了铜冶炼侧吹炉渣线部位侧墙镁铬砖的侵蚀损毁机制。结果表明:1)位于渣线处的镁铬砖由于受到铜锍、熔渣的交替冲刷、渗透作用,难以形成稳定的挂渣层,造成镁铬砖渗... 为了保证新工艺下侧吹炉的安全稳定运行,采用扫描电子显微镜、能谱仪分析了铜冶炼侧吹炉渣线部位侧墙镁铬砖的侵蚀损毁机制。结果表明:1)位于渣线处的镁铬砖由于受到铜锍、熔渣的交替冲刷、渗透作用,难以形成稳定的挂渣层,造成镁铬砖渗透-侵蚀-剥落的持续循环,导致该处的镁铬砖蚀损最为严重;而渣线上部镁铬砖的蚀损程度较小,原因是铜锍在渣线上部镁铬砖中的渗透作用明显减弱,镁铬砖热面形成稳定的尖晶石及橄榄石相致密层,可以一定程度上阻挡熔渣和铜锍的进一步渗透及侵蚀。2)铜锍虽然在镁铬砖中仅沿气孔和晶界渗透,并不参与侵蚀反应,但其渗透后包裹于基质颗粒或晶粒周围,破坏了镁铬砖的直接结合,破坏原镁铬砖的稳定结构,降低镁铬砖对熔渣及铜锍的抗侵蚀性。3)铜锍主要沿铬铁矿颗粒周围以及析出富铁尖晶石的方镁石晶间渗透,不利于镁铬砖抵抗SiO_(2)-FeO熔渣的渗透与侵蚀。 展开更多
关键词 铜冶炼 侧吹炉 镁铬砖 侵蚀 渗透 损毁机制
下载PDF
RH精炼炉用无铬耐火材料的研究现状和发展趋势 被引量:17
10
作者 周菲菲 邢方圆 +4 位作者 姜敏 张钊 鲁雄刚 李重河 金从进 《上海金属》 CAS 北大核心 2012年第3期33-38,共6页
镁铬砖由于具有良好的抗热震性和良好的抗渣性,而被广泛应用于冶炼、水泥等高温炉上。自上世纪80年代起,铬公害问题已受到人们的关注,于是开发替代镁铬材料的环境友好型无铬耐火材料成为当今研究的热点。针对当前无铬耐火材料存在的问题... 镁铬砖由于具有良好的抗热震性和良好的抗渣性,而被广泛应用于冶炼、水泥等高温炉上。自上世纪80年代起,铬公害问题已受到人们的关注,于是开发替代镁铬材料的环境友好型无铬耐火材料成为当今研究的热点。针对当前无铬耐火材料存在的问题,总结了各种无铬耐火材料的研究现状,并讨论了无铬耐火材料未来发展趋势和研究方向。 展开更多
关键词 RH精炼炉 无铬耐火材料 镁铬砖
下载PDF
宝钢RH精炼炉用耐火材料无铬化的实现 被引量:18
11
作者 赵明 陈荣荣 +1 位作者 沈钟铭 金从进 《耐火材料》 CAS 北大核心 2013年第6期433-436,共4页
介绍了宝钢RH炉内衬耐火材料无铬化工作及取得的成果,重点涉及下部槽、环流管和浸渍管部位无铬材料的开发应用过程。近年来,在RH槽体内壁上不断尝试了烧成镁尖晶石锆、刚玉-尖晶石和不烧镁尖晶石等材料,最终实现了以不烧镁尖晶石砖为主... 介绍了宝钢RH炉内衬耐火材料无铬化工作及取得的成果,重点涉及下部槽、环流管和浸渍管部位无铬材料的开发应用过程。近年来,在RH槽体内壁上不断尝试了烧成镁尖晶石锆、刚玉-尖晶石和不烧镁尖晶石等材料,最终实现了以不烧镁尖晶石砖为主体,结合部分刚玉-尖晶石浇注料整体浇注浸渍管的方案,实现了对RH浸渍管、环流管、下部槽和中上部槽等部位整槽镁铬质耐火材料的替代。工业应用试验表明,RH精炼炉的寿命业绩和成本消耗均获得进步,至2012年底,宝钢炼钢厂全面实现了RH精炼炉用无铬耐火材料的工业化应用。 展开更多
关键词 RH炉用耐火材料 镁铬砖 无铬化
下载PDF
纳米Fe_2O_3对镁铬耐火材料烧结及力学性能的影响 被引量:11
12
作者 赵惠忠 李红 +3 位作者 魏建修 汪厚植 慕松林 赵洪波 《耐火材料》 CAS 北大核心 2003年第5期256-258,共3页
在镁铬耐火材料中添加纳米Fe_2O_3,研究了它对镁铬耐火材料烧结性能与常温力学性能的影响。结果发现,在相同的工艺条件下,加入1%(外加)的纳米Fe_2O_3即可使镁铬砖的烧成温度降低150℃左右,并在相同烧成温度下能使试样的常温抗折强度和... 在镁铬耐火材料中添加纳米Fe_2O_3,研究了它对镁铬耐火材料烧结性能与常温力学性能的影响。结果发现,在相同的工艺条件下,加入1%(外加)的纳米Fe_2O_3即可使镁铬砖的烧成温度降低150℃左右,并在相同烧成温度下能使试样的常温抗折强度和耐压强度大幅度提高。分析认为,在镁铬耐火材料中添加少量纳米级Fe_2O_3,可促进MgO-FeO固溶体中Cr^(3+)和Al^(3+)含量的提高,增强镁铬砖的直接结合程度,从而提高其力学性能。 展开更多
关键词 纳米Fe2O3 镁铬耐火材料 烧结性能 力学性能
下载PDF
镁锆砖和镁铬砖的抗RH炉渣侵蚀性对比 被引量:8
13
作者 陈松林 孙加林 +3 位作者 熊小勇 薛文东 王健东 潘波 《耐火材料》 EI CAS 北大核心 2007年第6期417-420,423,共5页
为取代RH炉用镁铬材料,以电熔镁砂为主原料,分别加入单斜锆、脱硅锆、单斜锆与脱硅锆的混合粉、锆英石制备了ZrO2质量分数分别为15%和20%的镁锆砖,并利用静态坩埚法对比研究了镁锆砖和镁铬砖的抗RH炉渣侵蚀性。结果表明:对于Al2O3含量... 为取代RH炉用镁铬材料,以电熔镁砂为主原料,分别加入单斜锆、脱硅锆、单斜锆与脱硅锆的混合粉、锆英石制备了ZrO2质量分数分别为15%和20%的镁锆砖,并利用静态坩埚法对比研究了镁锆砖和镁铬砖的抗RH炉渣侵蚀性。结果表明:对于Al2O3含量高且碱度(CaO/SiO2比)大的RH炉渣,镁锆砖抗侵蚀性能优于镁铬砖的;镁锆砖的侵蚀机理是砖中的ZrO2与渣中的CaO迅速反应,形成高熔点物相CaZrO3,能堵塞砖中的孔隙而形成致密保护层,从而阻止钢渣对镁锆砖的进一步侵蚀;而镁铬砖的侵蚀机理是渣中的Al2O3、Fe2O3等R3+和镁铬尖晶石中Cr3+交换,渣与砖反应生成的镁铝尖晶石和镁铁尖晶石使得材料变性,同时由于体积效应使镁铬材料鼓胀开裂,从而导致镁铬砖的严重侵蚀。 展开更多
关键词 镁锆砖 镁铬砖 RH炉渣 侵蚀机理
下载PDF
粗铜对镁铬砖的侵蚀 被引量:9
14
作者 于仁红 陈开献 +1 位作者 李勇 蒋明学 《耐火材料》 CAS 北大核心 2002年第5期259-261,共3页
以贵溪冶炼厂PS卧式转炉 (15 0t)风口区使用后的残砖为样品 ,用化学分析、物理性能检验、EDAX和SEM等手段进行了分析研究。结果表明 :粗铜对镁铬耐火材料的侵蚀主要表现为渗透 ;粗铜渗透的主要途径为开口气孔 。
关键词 镁铬砖 转炉 粗铜 抗侵蚀性 渗透 冶炼 炉衬 耐火材料
下载PDF
废镁铬砖加入量对镁质浇注料性能的影响 被引量:7
15
作者 钟黎声 高里存 +1 位作者 马小斌 周婷 《硅酸盐通报》 CAS CSCD 北大核心 2009年第2期366-369,378,共5页
将回转窑烧成带废弃直接结合镁铬砖经过处理后,制成废镁铬砖再生料,用它替代镁质浇注料中的镁砂原料。文章研究了废镁铬砖的加入量对镁质浇注料性能的影响。结果表明:经过一定工艺处理后的废镁铬砖满足掺入要求,并且随着废砖加入量的增... 将回转窑烧成带废弃直接结合镁铬砖经过处理后,制成废镁铬砖再生料,用它替代镁质浇注料中的镁砂原料。文章研究了废镁铬砖的加入量对镁质浇注料性能的影响。结果表明:经过一定工艺处理后的废镁铬砖满足掺入要求,并且随着废砖加入量的增加,试样的烘干、高温和中温耐压强度、抗折强度、体积密度均逐渐增大。实验证明加入量为37%时,其性能指标接近对照试样,并对高温烧后试样进行了SEM及XRD分析。 展开更多
关键词 废弃镁铬砖 镁质浇注料 回收利用 烧结性能
下载PDF
镁铬砖在大型干法水泥回转窑烧成带的损毁 被引量:7
16
作者 云斯宁 章道运 +1 位作者 于仁红 蒋明学 《耐火材料》 CAS 北大核心 2004年第4期238-241,共4页
对 5 0 0 0t·d- 1干法水泥回转窑烧成带的用后直接结合镁铬砖 (LZMGe - 8A)进行了XRD、SEM和EDAX分析 ,观察了残砖显微结构的变化 ,探讨了其损毁机理。研究结果表明 :水泥熟料液相侵蚀引起砖热面的结构剥落 ;水泥原料及燃料中的钾... 对 5 0 0 0t·d- 1干法水泥回转窑烧成带的用后直接结合镁铬砖 (LZMGe - 8A)进行了XRD、SEM和EDAX分析 ,观察了残砖显微结构的变化 ,探讨了其损毁机理。研究结果表明 :水泥熟料液相侵蚀引起砖热面的结构剥落 ;水泥原料及燃料中的钾、钠、硫、氯化合物形成的碱盐以气相和液相形式进入砖的气孔内 ,随温度波动而液化或固化 ,并与砖反应导致砖的结构脆化 ,进而发生龟裂。因此 ,降低直接结合镁铬砖的显气孔率 ,并提高抗热震性 。 展开更多
关键词 直接结合镁铬砖 干法水泥回转窑烧成带 损毁 显微结构 结构剥落 龟裂 抗热震性 显气孔率 XRD分析 SEM分析 EDAX分析
下载PDF
炼铜诺兰达炉用镁铬砖损毁机理的探讨 被引量:9
17
作者 王继宝 梁永和 +2 位作者 李勇 舒旭波 曹友清 《耐火材料》 EI CAS 北大核心 2007年第1期74-76,79,共4页
简要介绍了诺兰达炉用耐火材料的现状,并以风口区使用后的镁铬残砖为试样,采用化学分析、SEM和EDAX等手段对其侵蚀机理进行了分析研究。结果表明:铜渣对镁铬耐火材料的侵蚀,在工作面以熔蚀为主;在砖体内部主要以锍渗透为主。锍渗透的主... 简要介绍了诺兰达炉用耐火材料的现状,并以风口区使用后的镁铬残砖为试样,采用化学分析、SEM和EDAX等手段对其侵蚀机理进行了分析研究。结果表明:铜渣对镁铬耐火材料的侵蚀,在工作面以熔蚀为主;在砖体内部主要以锍渗透为主。锍渗透的主要途径为开口气孔、晶界及微裂纹。 展开更多
关键词 诺兰达炉 镁铬砖 抗侵蚀性
下载PDF
铝铬砖和镁铬砖抗艾萨炉炉渣蚀损的模拟研究 被引量:6
18
作者 邹明 蒋明学 +1 位作者 钱跃进 史晓琪 《耐火材料》 EI CAS 北大核心 2007年第3期180-182,共3页
采用回转抗渣法模拟研究了试验温度、保温时间和熔渣加入量等因素对铝铬砖和镁铬砖抗艾萨炉炉渣侵蚀能力的影响。用SEM、EDAX及XRD等方法,对抗渣试样的显微结构和矿物组成进行了分析研究。结果表明:随着侵蚀温度的升高、保温时间的延长... 采用回转抗渣法模拟研究了试验温度、保温时间和熔渣加入量等因素对铝铬砖和镁铬砖抗艾萨炉炉渣侵蚀能力的影响。用SEM、EDAX及XRD等方法,对抗渣试样的显微结构和矿物组成进行了分析研究。结果表明:随着侵蚀温度的升高、保温时间的延长及炉渣加入量的增加,铝铬砖和镁铬砖的侵蚀面积增大;熔渣渗入铝铬砖后,形成铁铝尖晶石和铁铬尖晶石保护层,阻止了熔渣的侵蚀;三种耐火材料抗艾萨炉炉渣侵蚀能力由强到弱为:铝铬砖>电熔再结合镁铬砖>直接结合镁铬砖。 展开更多
关键词 艾萨炉 铝铬砖 镁铬砖 抗渣性 模拟试验
下载PDF
影响镁铬耐火材料抗粗铜侵蚀的因素 被引量:4
19
作者 陈开献 于仁红 +2 位作者 李勇 洪彦若 蒋明学 《耐火材料》 CAS 北大核心 2002年第2期92-94,共3页
研究了温度、保温时间、粗铜的加入量和气氛等因素对镁铬耐火材料抗粗铜侵蚀性能的影响。结果表明 :随着侵蚀温度的升高 ,侵蚀保温时间的延长和粗铜加入量的增加 ,其渗透面积增大 ;气氛对粗铜渗透性影响较大 ,粗铜熔体中 [O]浓度越高 ,... 研究了温度、保温时间、粗铜的加入量和气氛等因素对镁铬耐火材料抗粗铜侵蚀性能的影响。结果表明 :随着侵蚀温度的升高 ,侵蚀保温时间的延长和粗铜加入量的增加 ,其渗透面积增大 ;气氛对粗铜渗透性影响较大 ,粗铜熔体中 [O]浓度越高 ,粗铜的渗透性越强。 展开更多
关键词 镁铬耐火材料 抗粗铜侵蚀 影响因素 侵蚀性 渗透性
下载PDF
Al_2O_3对镁铬耐火材料致密化的影响 被引量:7
20
作者 戴淑平 严新林 +1 位作者 于景坤 高心魁 《材料与冶金学报》 CAS 2003年第4期262-265,共4页
为了提高镁铬耐火材料的烧结性能,通过考察气孔率、体积密度和常温耐压强度与Al2O3加入量之间的关系,讨论了Al2O3添加剂对两种不同镁铬耐火材料致密化的影响.结果表明,镁铬耐火材料的骨料不同,Al2O3对其烧结性能和致密化的影响也不一样.
关键词 镁铬耐火材料 电熔镁铬砂 三氧化二铝 致密化 烧结