The thermally stimulated shape memory behavior of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment molecular weight and hard segment content was investigated. The deformati...The thermally stimulated shape memory behavior of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment molecular weight and hard segment content was investigated. The deformation recovery ratio R-f of the EOBT samples increases with the soft segment molecular weight and the hard segment weight content, while the average overall deformation recovery speed V-r increases with the hard segment content. The temperature of maximum deformation recovery speed (T-M) is determined by the melting temperature of the soft segment crystals and the stability of the crystallized hard segment domains.展开更多
A series of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment length and hard segment content were synthesized. The compositional heterogeneity was studied by solvent extrac...A series of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment length and hard segment content were synthesized. The compositional heterogeneity was studied by solvent extraction. The results show that the compositional heterogeneity increases when soft segment length and hard segment content increase. The compositional heterogeneity is also reflected in the crystallization behavior and morphology of soft and hard segment in EOBT segmented copolymer. The more compositional heterogeneous the EOBT segmented copolymer is, the more different the morphology and the crystallization behavior between separated fractions. Compared with ethylene oxide-ethylene terephthalate (EOET) segmented copolymer, compositional heterogeneity in EOBT segmented copolymer is weaker. But the compositional heterogeneity in EOBT segmented copolymer with long soft segment and high hard segment content is still obvious.展开更多
文摘The thermally stimulated shape memory behavior of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment molecular weight and hard segment content was investigated. The deformation recovery ratio R-f of the EOBT samples increases with the soft segment molecular weight and the hard segment weight content, while the average overall deformation recovery speed V-r increases with the hard segment content. The temperature of maximum deformation recovery speed (T-M) is determined by the melting temperature of the soft segment crystals and the stability of the crystallized hard segment domains.
基金This work was supported by the National Natural Science Foundation of China and the National Key Projects for Fundamental Research"Macromolecule Condensed State",The State Science and TechnologyCommission of China.
文摘A series of ethylene oxide-butylene terephthalate (EOBT) segmented copolymers with different soft segment length and hard segment content were synthesized. The compositional heterogeneity was studied by solvent extraction. The results show that the compositional heterogeneity increases when soft segment length and hard segment content increase. The compositional heterogeneity is also reflected in the crystallization behavior and morphology of soft and hard segment in EOBT segmented copolymer. The more compositional heterogeneous the EOBT segmented copolymer is, the more different the morphology and the crystallization behavior between separated fractions. Compared with ethylene oxide-ethylene terephthalate (EOET) segmented copolymer, compositional heterogeneity in EOBT segmented copolymer is weaker. But the compositional heterogeneity in EOBT segmented copolymer with long soft segment and high hard segment content is still obvious.