期刊文献+
共找到865篇文章
< 1 2 44 >
每页显示 20 50 100
A review of linear friction welding of Ni -based superalloys 被引量:2
1
作者 Xiawei Yang Tingxi Meng +6 位作者 Qiang Chu Yu Su Zhenguo Guo Rui Xu Wenlong Fan Tiejun Ma Wenya Li 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第6期1382-1391,共10页
Ni-based superalloys are one of the most important materials employed in high-temperature applications within the aerospace and nuclear energy industries and in gas turbines due to their excellent corrosion,radiation,... Ni-based superalloys are one of the most important materials employed in high-temperature applications within the aerospace and nuclear energy industries and in gas turbines due to their excellent corrosion,radiation,fatigue resistance,and high-temperature strength.Linear friction welding(LFW)is a new joining technology with near-net-forming characteristics that can be used for the manu-facture and repair of a wide range of aerospace components.This paper reviews published works on LFW of Ni-based superalloys with the aim of understanding the characteristics of frictional heat generation and extrusion deformation,microstructures,mechanical proper-ties,flash morphology,residual stresses,creep,and fatigue of Ni-based superalloy weldments produced with LFW to enable future optim-um utilization of the LFW process. 展开更多
关键词 Ni-based superalloys linear friction welding MICROSTRUCTURES mechanical properties flash morphology
下载PDF
Effect of Ti and Ta content on the oxidation resistance of Co-Ni-based superalloys 被引量:1
2
作者 Yuheng Zhang Zixin Li +2 位作者 Yunwei Gui Huadong Fu Jianxin Xie 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第2期351-361,共11页
Co-Ni-based superalloys are known for their capability to function at elevated temperatures and superior hot corrosion and thermal fatigue resistance.Therefore,these alloys show potential as crucial high-temperature s... Co-Ni-based superalloys are known for their capability to function at elevated temperatures and superior hot corrosion and thermal fatigue resistance.Therefore,these alloys show potential as crucial high-temperature structural materials for aeroengine and gas turbine hot-end components.Our previous work elucidated the influence of Ti and Ta on the high-temperature mechanical properties of alloys.However,the intricate interaction among elements considerably affects the oxidation resistance of alloys.In this paper,Co-35Ni-10Al-2W-5Cr-2Mo-1Nb-xTi-(5−x)Ta alloys(x=1,2,3,4)with varying Ti and Ta contents were designed and compounded,and their oxidation resistance was investigated at the temperature range from 800 to 1000℃.After oxidation at three test conditions,namely,800℃for 200 h,900℃for 200 h,and 1000℃for 50 h,the main structure of the oxide layer of the alloy consisted of spinel,Cr_(2)O_(3),and Al_(2)O_(3)from outside to inside.Oxides consisting of Ta,W,and Mo formed below the Cr_(2)O_(3)layer.The interaction of Ti and Ta imparted the highest oxidation resistance to 3Ti2Ta alloy.Conversely,an excessive amount of Ti or Ta resulted in an adverse effect on the oxidation resistance of the alloys.This study reports the volatilization of W and Mo oxides during the oxidation process of Co-Ni-based cast superalloys with a high Al content for the first time and explains the formation mechanism of holes in the oxide layer.The results provide a basis for gaining insights into the effects of the interaction of alloying elements on the oxidation resistance of the alloys they form. 展开更多
关键词 Co-Ni-based superalloys high-temperature oxidation Ti and Ta elements formation mechanism of holes
下载PDF
Versatile fluidity test model for cast superalloys and comparison between IN718 and IN939
3
作者 Jun ZHANG Zi-qi JIE +1 位作者 Miao-nan LIU Min GUO 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2024年第9期2881-2888,共8页
A spiral fluidity test model of superalloys with 10 mm in height and 3 mm in thickness was designed to evaluate the fluidity of two distinct Ni-based superalloys IN718 and IN939.The factors influencing fluidity are as... A spiral fluidity test model of superalloys with 10 mm in height and 3 mm in thickness was designed to evaluate the fluidity of two distinct Ni-based superalloys IN718 and IN939.The factors influencing fluidity are ascertained through comparative analysis utilizing methodologies such as JMat Pro,differential scanning calorimetry and high-temperature confocal laser scanning microscopy.The results show that under identical testing conditions,the fluidity of the IN939 superalloy surpasses that of the IN718 superalloy.When subjected to the same temperature,the melt viscosity and surface tension of IN939 superalloy are considerably reduced relative to those of IN718 superalloy,which is beneficial to improving the melt fluidity.Furthermore,the liquidus temperature and solidification range for the IN939 superalloy are both smaller compared with those of the IN718 superalloy.This condition proves advantageous in delaying dendrite coherency,thereby improving fluidity. 展开更多
关键词 FLUIDITY solidification range superalloys surface tension VISCOSITY
下载PDF
Recent research progress in the mechanism and suppression of fusion welding-induced liquation cracking of nickel based superalloys 被引量:1
4
作者 Zongli Yi Jiguo Shan +2 位作者 Yue Zhao Zhenlin Zhang Aiping Wu 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2024年第5期1072-1088,共17页
Nickel-based superalloys are extensively used in the crucial hot-section components of industrial gas turbines,aeronautics,and astronautics because of their excellent mechanical properties and corrosion resistance at ... Nickel-based superalloys are extensively used in the crucial hot-section components of industrial gas turbines,aeronautics,and astronautics because of their excellent mechanical properties and corrosion resistance at high temperatures.Fusion welding serves as an effective means for joining and repairing these alloys;however,fusion welding-induced liquation cracking has been a challenging issue.This paper comprehensively reviewed recent liquation cracking,discussing the formation mechanisms,cracking criteria,and remedies.In recent investigations,regulating material composition,changing the preweld heat treatment of the base metal,optimizing the welding process parameters,and applying auxiliary control methods are effective strategies for mitigating cracks.To promote the application of nickel-based superalloys,further research on the combination impact of multiple elements on cracking prevention and specific quantitative criteria for liquation cracking is necessary. 展开更多
关键词 nickel-based superalloy fusion welding liquation cracking cracking mechanism cracking suppression
下载PDF
Additive manufacturing of Ni-based superalloys: Residual stress, mechanisms of crack formation and strategies for crack inhibition 被引量:9
5
作者 Chuan Guo Gan Li +8 位作者 Sheng Li Xiaogang Hu Hongxing Lu Xinggang Li Zhen Xu Yuhan Chen Qingqing Li Jian Lu Qiang Zhu 《Nano Materials Science》 EI CAS CSCD 2023年第1期53-77,共25页
The additive manufacturing(AM)of Ni-based superalloys has attracted extensive interest from both academia and industry due to its unique capabilities to fabricate complex and high-performance components for use in hig... The additive manufacturing(AM)of Ni-based superalloys has attracted extensive interest from both academia and industry due to its unique capabilities to fabricate complex and high-performance components for use in high-end industrial systems.However,the intense temperature gradient induced by the rapid heating and cooling processes of AM can generate high levels of residual stress and metastable chemical and structural states,inevitably leading to severe metallurgical defects in Ni-based superalloys.Cracks are the greatest threat to these materials’integrity as they can rapidly propagate and thereby cause sudden and non-predictable failure.Consequently,there is a need for a deeper understanding of residual stress and cracking mechanisms in additively manufactured Ni-based superalloys and ways to potentially prevent cracking,as this knowledge will enable the wider application of these unique materials.To this end,this paper comprehensively reviews the residual stress and the various mechanisms of crack formation in Ni-based superalloys during AM.In addition,several common methods for inhibiting crack formation are presented to assist the research community to develop methods for the fabrication of crack-free additively manufactured components. 展开更多
关键词 Additive manufacturing Ni-based superalloys Residual stress Mechanisms of crack formation Methods of crack inhibition
下载PDF
On establishment of novel constitutive model for directionally solidified nickel-based superalloys utilizing machine learning methods
6
作者 Jia-yan Sun Rong Yin +2 位作者 Ye-yuan Hu Yun-xiang Tan Qing-yan Xu 《China Foundry》 SCIE CAS CSCD 2023年第5期365-375,共11页
To enhance the accuracy of mechanical simulation in the directional solidification process of turbine blades for heavy-duty gas turbines,a new constitutive model that employs machine learning methods was developed.Thi... To enhance the accuracy of mechanical simulation in the directional solidification process of turbine blades for heavy-duty gas turbines,a new constitutive model that employs machine learning methods was developed.This model incorporates incremental learning and transfer learning,thus improves the predictive accuracy and generalization performance.To account for the anisotropy of the directionally solidified alloy,a deformation direction parameter is added to the model,enabling prediction of the stress-strain relationship of the alloy under different deformation directions.The predictive capabilities of both models are evaluated using correlation coefficient(R),average relative error(δ),and value of relative error(RE).Compared to the traditional model,the machine learning constitutive model achieves higher prediction accuracy and better generalization performance.This offers a new approach for the establishment of flow constitutive models for other directionally solidified and single-crystal superalloys. 展开更多
关键词 Ni-based superalloy constitutive model machine learning directional solidification ANISOTROPY
下载PDF
Effect of carbon and boron additions on segregation behavior of directionally solidified nickel-base superalloys with rhenium 被引量:7
7
作者 胡勤 刘林 +3 位作者 赵新宝 高斯峰 张军 傅恒志 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第11期3257-3264,共8页
The phase transformation temperature, segregation behavior of elements and as-cast microstructure were investigated in experimental nickel-base superalloys with different levels of carbon and boron. The results show t... The phase transformation temperature, segregation behavior of elements and as-cast microstructure were investigated in experimental nickel-base superalloys with different levels of carbon and boron. The results show that the liquidus temperature decreases gradually but the carbide solvus temperature increases obviously with increasing carbon addition. Minor boron addition to the alloy decreases the liquidus temperature, carbide solvus temperature and solidus temperature slightly. Apart from rhenium, the segregation coefficients of the elements alter insignificantly with the addition of carbon. The segregation behavior of rhenium, tungsten and tantalum become more severe with boron addition. The volume fraction and size of primary carbides increase with increasing carbon addition. The main morphology of the carbides is script-like in the alloys with carbon addition while the carbide sheets tend to be concentrated and coarse in the boron-containing alloys 展开更多
关键词 CARBON BORON segregation behavior directional solidification nickel-base superalloys
下载PDF
Solidification characteristics and hot tearing susceptibility of Ni-based superalloys for turbocharger turbine wheel 被引量:3
8
作者 石照夏 董建新 +1 位作者 张麦仓 郑磊 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2014年第9期2737-2751,共15页
The solidification characteristics and the hot tearing susceptibility were investigated on two Ni-based superalloys for turbocharger turbine wheel, K418 and K419. The segregation behaviors of the alloying elements and... The solidification characteristics and the hot tearing susceptibility were investigated on two Ni-based superalloys for turbocharger turbine wheel, K418 and K419. The segregation behaviors of the alloying elements and the precipitation phases were also studied. The results show that the solidification behavior of K419 alloy is complicated when compared with K418 due to the interdendritic segregation of many kinds of strong interdendritic partitioning elements in the remaining liquid at the final stage of solidification. The segregation of multiple elements in interdendritic liquid results in an extremely low solidus in K419. A long residual liquid stage is found during the solidification of K419, giving rise to reduced cohesion strength of dendrites and increased sensitivity to hot tearing. A hot tearing susceptibility coefficient(HTS) criterion is proposed based on a hot tearing sensitive model. The HTS value of K419 alloy is larger than that of K418 alloy. 展开更多
关键词 SOLIDIFICATION hot tearing susceptibility Ni-based superalloys SEGREGATION
下载PDF
COMPUTER SIMULATION OF GRAIN BOUNDARY SEGREGATION BEHAVIOR AND MECHANISMS OF STRENGTHENING OF Mg IN Ni-BASED SUPERALLOYS 被引量:2
9
作者 陈国良 葛红林 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 1995年第2期108+84-91,共9页
This paper used EAM and static relaxation method to simulate the grain boundary segregation behavior of Mg in Ni-based superalloys. The results offer a better understanding in the strengthening mechanism of Mg additio... This paper used EAM and static relaxation method to simulate the grain boundary segregation behavior of Mg in Ni-based superalloys. The results offer a better understanding in the strengthening mechanism of Mg addition in superalloys. The segregation of Mg increases the grain boundary cohesive bond and the vacancy formation energy, and decreases the mobility of grain boundary dislocation. It results in the retardation of creep voids initiation and growth. 展开更多
关键词 Mg in superalloys Grain boundary segregation SUPERALLOY computer Simulation
下载PDF
PROPERTIES, WELDABILITY AND APPLICATIONS OF ADVANCED WROUGHT SUPERALLOYS FOR GAS TURBINE ENGINES 被引量:4
10
作者 D.L. Klarstrom V.R. Ishwar M.D. Rowe 《Acta Metallurgica Sinica(English Letters)》 SCIE EI CAS CSCD 2005年第1期1-14,共14页
Alloy selection and alloy design both require consideration of an array of material attributes, including in-service properties, weldability and fabricability. Critical properties of advanced wrought superalloys for g... Alloy selection and alloy design both require consideration of an array of material attributes, including in-service properties, weldability and fabricability. Critical properties of advanced wrought superalloys for gas turbine applications include high temperature strength, thermal stability, oxidation resistance and fatigue resistance. In this paper, the properties of twelve wrought solid-solution-strengthened and six age-hardenable superalloys are compared. Weldability is an important attribute and can be a major limiting factor in the use of certain alloys. Weldability test methods are discussed and the resistance of alloys to solidification cracking and strain-age cracking is compared. The use of weldability testing in the development of modern wrought su-peralloys is discussed with several examples cited. Finally, alloy selection for gas turbine components is outlined, taking into account both alloy properties and fabricability. 展开更多
关键词 wrought superalloys mechanical properties strain-age cracking of weldments selection and application of wrought superalloys
下载PDF
Effect of ruthenium on γ' precipitation behavior and evolution in single crystal superalloys 被引量:4
11
作者 刘丽荣 金涛 +2 位作者 刘金来 孙晓峰 胡壮麒 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2013年第1期14-22,共9页
The effect of Ru on γ' precipitation behavior and evolution in single crystal superalloys with different Ru contents were investigated by scanning electron microscopy with energy dispersive spectroscopy,3D atomic pr... The effect of Ru on γ' precipitation behavior and evolution in single crystal superalloys with different Ru contents were investigated by scanning electron microscopy with energy dispersive spectroscopy,3D atomic probing,differential scanning calorimetry.The results show that the solvus of the γ' phase decreases gradually with increasing Ru content in the alloys by casting or by the same solution and aging treatments,the alloy with a larger Ru content yields a smaller γ' phase.The addition of Ru increases the growth rate and coarsening rate of the γ' phase.Ru mainly distributes in the γ phase,which causes more Re and Mo partition into the γ' phase,increasing the absolute value of mismatch and the rafting rate of the γ' phase. 展开更多
关键词 single crystal superalloy RUTHENIUM gamma prime PRECIPITATION growth rate coarsening rate MISMATCH
下载PDF
Oxidation behaviors of wrought nickel-based superalloys in various high temperature environments 被引量:9
12
作者 Changheui JANG Daejong KIM +3 位作者 Donghoon KIM Injin SAH Woo-Seog RYU Young-sung YOO 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2011年第7期1524-1531,共8页
Oxidation characteristics of Alloy 617 and Haynes 230 at 900 oC in simulated helium environment,hot steam environment containing H2 as well as in air and pure helium conditions were investigated.Compared to air condit... Oxidation characteristics of Alloy 617 and Haynes 230 at 900 oC in simulated helium environment,hot steam environment containing H2 as well as in air and pure helium conditions were investigated.Compared to air condition,the oxidation rate of Alloy 617 was not significantly affected in helium and hot steam environments,while Haynes 230 showed lower oxidation rate in helium environment.On the other hand,the oxide morphology and structure of Alloy 617 were strongly affected by the environments,but those of Haynes 230 were less dependent on the environments.For Haynes 230,a Cr2O3 inner layer and a protective MnCr2O4 outer layer were formed in all environments,which contributed to the better oxidation resistance.As the mechanical properties,such as creep and tensile properties,were significantly affected by the oxidation behaviors,surface treatment methods to enhance oxidation resistance of these alloys should be developed. 展开更多
关键词 oxidation nickel-based superalloys very high temperature reactor (VHTR) impure helium hot steam
下载PDF
Identification of Iron Oxides Qualitatively/Quantitatively Formed during the High Temperature Oxidation of Superalloys in Air and Steam Environments 被引量:6
13
作者 M. Siddique N. Hussain M. Shafi 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2009年第4期479-482,共4页
Mossbauer spectroscopy has been used to study the morphology of iron oxides formed during the oxidation of superalloys, such as SS-304L (1.4306S), Incoloy-800H, Incoloy-825, UBHA-25L, Sanicro-28 and Inconel-690, at ... Mossbauer spectroscopy has been used to study the morphology of iron oxides formed during the oxidation of superalloys, such as SS-304L (1.4306S), Incoloy-800H, Incoloy-825, UBHA-25L, Sanicro-28 and Inconel-690, at 1200℃ exposed in air and steam environments for 400 h. The basic aim was to identify and compare the iron oxides qualitatively and quantitatively, formed during the oxidation of these alloys in two environments. The behaviour of alloy UBHA-25L in high temperature oxidation in both environments indicates that it has good oxidation resistance especially in steam, whereas Sanicro-28 has excellent corrosion resistance in steam environment. In air oxidation of Inconel-690 no iron oxide, with established Mossbauer parameters, was detected. 展开更多
关键词 superalloys Mossbauer spectroscopy OXIDATION Corrosion products
下载PDF
Effect of Co on oxidation and hot corrosion behavior of two nickel-based superalloys under Na_(2)SO_(4)-NaCl at 900℃ 被引量:6
14
作者 Jun-sheng MENG Ming-xuan CHEN +1 位作者 Xiao-ping SHI Qiang MA 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2021年第8期2402-2414,共13页
Nickel-based superalloys with and without Co by partial replacement of W were prepared using double vacuum melting.A comparison of the oxidation in air and hot corrosion behaviors under molten 75 wt.%Na2 SO4+25 wt.%Na... Nickel-based superalloys with and without Co by partial replacement of W were prepared using double vacuum melting.A comparison of the oxidation in air and hot corrosion behaviors under molten 75 wt.%Na2 SO4+25 wt.%NaCl at 900℃were systematically investigated.The results showed that partial replacement of W with Co promoted the formation of chromia scale and consequently decreased the oxidation rate.Besides,the addition of Co also retarded the internal oxidation/nitridation of Al and consequently promoted the growth of Al_(2) O3 scale,which further decreased the scaling rate and improved the adhesion of scale.Moreover,the addition of Co also further improved the hot corrosion resistance under molten Na2 SO4-NaCl salts. 展开更多
关键词 nickel based superalloys OXIDATION hot corrosion spallation resistance
下载PDF
First-principles calculations for the elastic properties of Ni-base model superalloys: Ni/Ni_3Al multilayers 被引量:5
15
作者 王云江 王崇愚 《Chinese Physics B》 SCIE EI CAS CSCD 2009年第10期4339-4348,共10页
A model system consisting of Ni[001](100)/Ni3Al[001](100) multi-layers are studied using the density functional theory in order to explore the elastic properties of single crystal Ni-based superalloys. Simulation ... A model system consisting of Ni[001](100)/Ni3Al[001](100) multi-layers are studied using the density functional theory in order to explore the elastic properties of single crystal Ni-based superalloys. Simulation results are consistent with the experimental observation that rafted Ni-base superalloys virtually possess a cubic symmetry. The convergence of the elastic properties with respect to the thickness of the multilayers are tested by a series of multilayers from 2γ′+2γto 10γ′+10γ atomic layers. The elastic properties are found to vary little with the increase of the multilayer's thickness. A Ni/Ni3Al multilayer with 10γ′+10γ atomic layers (3.54 nm) can be used to simulate the mechanical properties of Ni-base model superalloys. Our calculated elastic constants, bulk modulus, orientation-dependent shear modulus and Young's modulus, as well as the Zener anisotropy factor are all compatible with the measured results of Ni-base model superalloys R1 and the advanced commercial superalloys TMS-26, CMSX-4 at a low temperature. The mechanical properties as a function of the γ′ phase volume fraction are calculated by varying the proportion of the γ and γ′ phase in the multilayers. Besides, the mechanical properties of two-phase Ni/Ni3Al multilayer can be well predicted by the Voigt-Reuss-Hill rule of mixtures. 展开更多
关键词 Ni-based superalloys Ni/Ni3Al multilayer mechanical property first principles rule of mixture
下载PDF
Hot deformation behavior of FGH96 superalloys 被引量:4
16
作者 Jiantao Liu Guoquan Liu +3 位作者 Benfu Hu Yuepeng Song Ziran Qin Yiwen Zhang 《Journal of University of Science and Technology Beijing》 CSCD 2006年第4期319-323,共5页
The hot deformation behavior of FGH96 superalloys at 1070-1170℃ and 5×10^-4-2×10^-1 s^-1 were investigated by means of the isothermal compression tests at a Gleeble-1500 thermal mechanical simulator. The re... The hot deformation behavior of FGH96 superalloys at 1070-1170℃ and 5×10^-4-2×10^-1 s^-1 were investigated by means of the isothermal compression tests at a Gleeble-1500 thermal mechanical simulator. The results show that dynamic recovery acts as the main softening mechanism below 2×10^-3 s^-1, whereas dynamic recrystallization acts as the main softening mechanism above 2× 10^-3 s^-1 during deformation; the temperature increase caused by the deformation and the corresponding softening stress is negligible; the thermal-mechanical constitutive model to describe the hot deformation behavior is given, and the value of the apparent deformation activation energy (Qdef) is determined to be 354.93 kJ/mol. 展开更多
关键词 FGH96 superalloys hot deformation hot deformation activation energy dynamic recovery dynamic recrystallization
下载PDF
Activity coefficients of NiO and CoO in CaO–Al_2O_3–SiO_2 slag and their application to the recycling of Ni–Co–Fe-based end-of-life superalloys via remelting 被引量:2
17
作者 Xin Lu Takahiro Miki Tetsuya Nagasaka 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2017年第1期25-36,共12页
To design optimal pyrometallurgical processes for nickel and cobalt recycling, and more particularly for the end-of-life process of Ni-Co-Fe-based end-of-life(EoL) superalloys, knowledge of their activity coefficien... To design optimal pyrometallurgical processes for nickel and cobalt recycling, and more particularly for the end-of-life process of Ni-Co-Fe-based end-of-life(EoL) superalloys, knowledge of their activity coefficients in slags is essential. In this study, the activity coefficients of NiO and CoO in CaO-Al_2O_3-SiO_2 slag, a candidate slag used for the EoL superalloy remelting process, were measured using gas/slag/metal equilibrium experiments. These activity coefficients were then used to consider the recycling efficiency of nickel and cobalt by remelting EoL superalloys using CaO-Al_2O_3-SiO_2 slag. The activity coefficients of NiO and CoO in CaO-Al_2O_3-SiO_2 slag both show a positive deviation from Raoult's law, with values that vary from 1 to 5 depending on the change in basicity. The activity coefficients of NiO and CoO peak in the slag with a composition near B =(%CaO)/(%SiO_2) = 1, where B is the basicity. We observed that controlling the slag composition at approximately B = 1 effectively reduces the cobalt and nickel oxidation losses and promotes the oxidation removal of iron during the remelting process of EoL superalloys. 展开更多
关键词 RECYCLING nickel cobalt END-OF-LIFE superalloys activity coefficients REMELTING SLAG
下载PDF
HOT CORROSION BEHAVIOR OF Ni-BASED SUPERALLOYS WITH HIGHER Cr CONTENTS -PART Ⅱ.MECHANISM OF HOT CORROSION BEHAVIOR 被引量:1
18
作者 崔华 张济山 +2 位作者 村田纯教 森永正彦 汤川夏夫 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 1996年第2期98+91-98,共9页
Based on the experimental results in the previous paper, the mechanism of the hot corrosion behavior of alloy system Ni-16Cr-gAl-2W- 1Mo-4Co-(0~4)Ti-f(0 ~ 4)Ta-(0~4)Nb (in at%) is investigated. In the Ti and Nb-ric... Based on the experimental results in the previous paper, the mechanism of the hot corrosion behavior of alloy system Ni-16Cr-gAl-2W- 1Mo-4Co-(0~4)Ti-f(0 ~ 4)Ta-(0~4)Nb (in at%) is investigated. In the Ti and Nb-rich corners, hot corrosion is controlled by the basic fluxing mechanism, and a dense and protective surface scale is formed which results in the better hot corrosion resistance for the alloys in these regions. While in the Ta-rich comer,the basic and acidic mechanisms function alternatively, which results in the catastrophic corrosion by forming the porous and non-protective scale, so the alloys in this region show poor hot corrosion resistance. In addition, the concept of 'effective chromium content' seemed to give a correct prediction of the hot corrosion resistance of such alloy systems. 展开更多
关键词 hot corrosion SUPERALLOY alloying effects
下载PDF
An anisotropic micromechanics model for predicting the rafting direction in Ni-based single crystal superalloys 被引量:2
19
作者 Shuang-Yu Li Wen-Ping Wu Ming-Xiang Chen 《Acta Mechanica Sinica》 SCIE EI CAS CSCD 2016年第1期135-143,共9页
An anisotropic micromechanics model based on the equivalent inclusion method is developed to investigate the rafting direction of Ni-based single crystal superalloys. The micromechanical model considers actual cubic s... An anisotropic micromechanics model based on the equivalent inclusion method is developed to investigate the rafting direction of Ni-based single crystal superalloys. The micromechanical model considers actual cubic structure and orthogonal anisotropy properties. The von Mises stress, elastic strain energy density, and hydrostatic pressure in dif- ferent inclusions of micromechanical model are calculated when applying a tensile or compressive loading along the [001] direction. The calculated results can successfully pre- dict the rafting direction for alloys exhibiting a positive or a negative mismatch, which are in agreement with pervious experimental and theoretical studies. Moreover, the elastic constant differences and mismatch degree of the matrix and precipitate phases and their influences on the rafting direction are carefully discussed. 展开更多
关键词 Ni-based single crystal superalloys RAFTING Equivalent inclusion theory Stroh formalism
下载PDF
New approach for assessing the weldability of precipitation-strengthened nickel-base superalloys 被引量:1
20
作者 Homam Naffakh Moosavy Mohammad-Reza Aboutalebi +2 位作者 Seyed Hossein Seyedein Meisam Khodabakhshi Carlo Mapelli 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2013年第12期1183-1191,共9页
A new procedure was proposed for evaluating the weldability of nickel-base superalloys. The theory is on the basis of two microstructural patterns. In pattern I, the weld microstructure exhibits severe alloying segreg... A new procedure was proposed for evaluating the weldability of nickel-base superalloys. The theory is on the basis of two microstructural patterns. In pattern I, the weld microstructure exhibits severe alloying segregation, many low-melting eutectic structures, and low weldability. The weld requires a weaker etchant and a shorter time for etching. In pattern Ⅱ, the weld microstructure displays less alloying segregation, low quantity of eutectic structures, and high weldability. The weld needs a stronger etchant and a longer time for etching. Five superalloys containing different amounts of Nb and Ti were designed to verify the patterns. After welding operations, the welds were etched by four etchants with different corrosivities. The weldability was determined by TG-DSC measurements. The metallography and weldability results confirmed the theoretic patterns. Finally, the etchant corrosivity and etching time were proposed as new criteria to evaluate the weldability of nickel-base superalloys. 展开更多
关键词 superalloys nickel alloys WELDABILITY METALLOGRAPHY ETCHING segregution EUTECTICS
下载PDF
上一页 1 2 44 下一页 到第
使用帮助 返回顶部