Amphoteric polyacrylamide was prepared first by the copolymerization of acrylamide with sodium acrylate and then through Mannich reaction.The copolymerization was carried out with a redox initiation system using the ...Amphoteric polyacrylamide was prepared first by the copolymerization of acrylamide with sodium acrylate and then through Mannich reaction.The copolymerization was carried out with a redox initiation system using the method of inverse emulsion polymerization.In this paper the reaction conditions and factors that affect emulsion stability were studied.Experiments show that a stable latex can be obtained under the following conditions:anionic degree is five percent,the ratio among acrylamide,formaldehyde and dimethylamine is 1∶1∶1.2,reaction temperature is 45 ℃,reaction time lasts four hours,and pH equals 5.0.The amphoteric copolymer has a higher molecular weight and cationic degree,so it is an ideal filler retention and drainage aid in paper making.展开更多
文摘Amphoteric polyacrylamide was prepared first by the copolymerization of acrylamide with sodium acrylate and then through Mannich reaction.The copolymerization was carried out with a redox initiation system using the method of inverse emulsion polymerization.In this paper the reaction conditions and factors that affect emulsion stability were studied.Experiments show that a stable latex can be obtained under the following conditions:anionic degree is five percent,the ratio among acrylamide,formaldehyde and dimethylamine is 1∶1∶1.2,reaction temperature is 45 ℃,reaction time lasts four hours,and pH equals 5.0.The amphoteric copolymer has a higher molecular weight and cationic degree,so it is an ideal filler retention and drainage aid in paper making.