By testing a substantial number of tripler and z-cut KDP and DKDP crystals, we have observed that at 355nm, the laser induced damage threshold in the R-on-one test is higher than that in the one-on-one test. It is pro...By testing a substantial number of tripler and z-cut KDP and DKDP crystals, we have observed that at 355nm, the laser induced damage threshold in the R-on-one test is higher than that in the one-on-one test. It is proved that laser conditioning is an efficient way to improve the damage resistance. The efficiency of laser conditioning becomes increasingly good with smaller ramping fluence steps. We have also found that the damage resistance of the z-cut crystal is higher than the triplet cut, and the pinpoint number is definitely less in the z-cut crystal. The reason for these observations is discussed.展开更多
We present the characteristics of bulk damage induced by the third harmonic of Nd:YAG laser irradiation in KDP and DKDP crystals. Bulk damage occurs as a few or a series of pinpoints consisting of a core and the defo...We present the characteristics of bulk damage induced by the third harmonic of Nd:YAG laser irradiation in KDP and DKDP crystals. Bulk damage occurs as a few or a series of pinpoints consisting of a core and the deforming zone. The results of a 1-on-1 test reveal that the pinpoint size increases with incvreasing fluence, and the pinpoint density increases exponentially with increasing fluence. The results of an s-on-1 test indicate that the pinpoint density increases gradually with laser pulse number, but the size does not grow. These results are consistent with a model in which nanoabsorbers are assumed to exist in the crystal and the initiation of damage is determined by heating them to the critical temperature.展开更多
A thermal model is considered in order to better understand the mechanism of laser induced damage in KDP and DKDP crystals. We demonstrate that the expressions of pinpoint density and damage probability, predicted by ...A thermal model is considered in order to better understand the mechanism of laser induced damage in KDP and DKDP crystals. We demonstrate that the expressions of pinpoint density and damage probability, predicted by the thermal model, are consistent with the experimental data. We also discuss the effect of particle interaction on the thermal model.展开更多
By testing the number increase and size growth of surface and bulk laser induced damage in KDP and DKDP crystals, we observe different growth characteristics of surface and bulk damage under multiple 355nm laser irrad...By testing the number increase and size growth of surface and bulk laser induced damage in KDP and DKDP crystals, we observe different growth characteristics of surface and bulk damage under multiple 355nm laser irradiations. The size of the surface damage grows exponentially, but that of the bulk damage does not grow. In contrast, the bulk damage number increases, but that of surface damage does not increase significantly. We attribute the differences to the different formation of the damage initiators and the different damage testing volumes.展开更多
KDP crystals doped with Chicago Sky Blue 6B(CSB-6B) were grown by traditional lowering temperature method.The optical properties and structural perfection of KDP crystals were investigated by transmittance spectra a...KDP crystals doped with Chicago Sky Blue 6B(CSB-6B) were grown by traditional lowering temperature method.The optical properties and structural perfection of KDP crystals were investigated by transmittance spectra and high-resolution X-ray diffraction,respectively.The results indicate that CSB-6B tends to be incorporated into the pyramidal sector of KDP crystals(PyS-KDP) and lead to inclusions parallel to(101) face.Additionally,the transmittance of as-grown KDP crystals decreases as the amount of CSB-6B increases. Moreover,the rocking curves of PyS-KDP suggest that CSB-6B can deteriorate the structural perfection of PyS-KDP.展开更多
基金Supported by the National Natural Science Foundation of China under Grant No 10676019.
文摘By testing a substantial number of tripler and z-cut KDP and DKDP crystals, we have observed that at 355nm, the laser induced damage threshold in the R-on-one test is higher than that in the one-on-one test. It is proved that laser conditioning is an efficient way to improve the damage resistance. The efficiency of laser conditioning becomes increasingly good with smaller ramping fluence steps. We have also found that the damage resistance of the z-cut crystal is higher than the triplet cut, and the pinpoint number is definitely less in the z-cut crystal. The reason for these observations is discussed.
基金Supported by the National Natural Science Foundation of China under Grant No 10676019.
文摘We present the characteristics of bulk damage induced by the third harmonic of Nd:YAG laser irradiation in KDP and DKDP crystals. Bulk damage occurs as a few or a series of pinpoints consisting of a core and the deforming zone. The results of a 1-on-1 test reveal that the pinpoint size increases with incvreasing fluence, and the pinpoint density increases exponentially with increasing fluence. The results of an s-on-1 test indicate that the pinpoint density increases gradually with laser pulse number, but the size does not grow. These results are consistent with a model in which nanoabsorbers are assumed to exist in the crystal and the initiation of damage is determined by heating them to the critical temperature.
基金Supported by the National Natural Science Foundation of China under Grant No 10676019.
文摘A thermal model is considered in order to better understand the mechanism of laser induced damage in KDP and DKDP crystals. We demonstrate that the expressions of pinpoint density and damage probability, predicted by the thermal model, are consistent with the experimental data. We also discuss the effect of particle interaction on the thermal model.
基金Supported by the National Natural Science Foundation of China under Grant No 10676019
文摘By testing the number increase and size growth of surface and bulk laser induced damage in KDP and DKDP crystals, we observe different growth characteristics of surface and bulk damage under multiple 355nm laser irradiations. The size of the surface damage grows exponentially, but that of the bulk damage does not grow. In contrast, the bulk damage number increases, but that of surface damage does not increase significantly. We attribute the differences to the different formation of the damage initiators and the different damage testing volumes.
基金Supported by the State High Technology Program for Inertial Confinement Fusion and National Natural Science Foundation of China (No 59823003, 50721002)China Postdoctoral Science Foundation (No 20080441139)Youth Scientist Fund of Shandong Province (No 2004BS04022)
文摘KDP crystals doped with Chicago Sky Blue 6B(CSB-6B) were grown by traditional lowering temperature method.The optical properties and structural perfection of KDP crystals were investigated by transmittance spectra and high-resolution X-ray diffraction,respectively.The results indicate that CSB-6B tends to be incorporated into the pyramidal sector of KDP crystals(PyS-KDP) and lead to inclusions parallel to(101) face.Additionally,the transmittance of as-grown KDP crystals decreases as the amount of CSB-6B increases. Moreover,the rocking curves of PyS-KDP suggest that CSB-6B can deteriorate the structural perfection of PyS-KDP.