To efficiently co-extract Ni and Cu from low-grade nickel-copper sulfide ore,chlorination roasting with NH;Cl followed by a water leaching process was investigated.The results show that 98.4%Ni and 98.5%Cu can be sync...To efficiently co-extract Ni and Cu from low-grade nickel-copper sulfide ore,chlorination roasting with NH;Cl followed by a water leaching process was investigated.The results show that 98.4%Ni and 98.5%Cu can be synchronously extracted when the ore particle size is 75-80μm,the roasting time is 2 h,the mass ratio of NH;Cl to ore is 1.6:1 and the roasting temperature is 550°C.The evolution behavior of various minerals was elucidated using X-ray diffraction(XRD)coupled with scanning electron microscopy(SEM).The kinetics of the chlorination process based on the differential thermal and thermogravimetric analysis(DTA-TG)data was analyzed by Kissinger method and Flynn-Wall-Ozawa(FWO)method.The chlorination process of low-grade nickel-copper sulfide ore mainly contains two stages:the decomposition of NH;Cl and the chlorination of ore.The maximum apparent activation energies(Ea)at two stages are determined to be 114.8 and 144.6 kJ/mol,respectively.The condensed product of exhaust gas is determined to be ammonium chloride,which can be recycled as the reactant again,making the process economic and clean.展开更多
基金the National Natural Science Foundation of China(No.52074069)the Natural Science Foundation of Hebei Province(No.E2020501022)+1 种基金the National Basic Research Program of China(No.2014CB643405)the Fundamental Research Funds for the Central Universities,China(No.N2223027)。
文摘To efficiently co-extract Ni and Cu from low-grade nickel-copper sulfide ore,chlorination roasting with NH;Cl followed by a water leaching process was investigated.The results show that 98.4%Ni and 98.5%Cu can be synchronously extracted when the ore particle size is 75-80μm,the roasting time is 2 h,the mass ratio of NH;Cl to ore is 1.6:1 and the roasting temperature is 550°C.The evolution behavior of various minerals was elucidated using X-ray diffraction(XRD)coupled with scanning electron microscopy(SEM).The kinetics of the chlorination process based on the differential thermal and thermogravimetric analysis(DTA-TG)data was analyzed by Kissinger method and Flynn-Wall-Ozawa(FWO)method.The chlorination process of low-grade nickel-copper sulfide ore mainly contains two stages:the decomposition of NH;Cl and the chlorination of ore.The maximum apparent activation energies(Ea)at two stages are determined to be 114.8 and 144.6 kJ/mol,respectively.The condensed product of exhaust gas is determined to be ammonium chloride,which can be recycled as the reactant again,making the process economic and clean.