The sintering conditions of artificial lightmass aggregate (LWA) made up of sewage sludge,clay and pulverized flyash (PFA) by trefoil rotary kiln were investigated. The influencing factors of the aggregate strength in...The sintering conditions of artificial lightmass aggregate (LWA) made up of sewage sludge,clay and pulverized flyash (PFA) by trefoil rotary kiln were investigated. The influencing factors of the aggregate strength including furnace temperature when feeding,the heating-up time from 500 to 1 000 ℃ ,the highest burning temperature,retention time at the highest burning temperature and furnace temperature at burning end were analyzed by orthogonal tests. The results show that 44.4% (mass fraction) sewage sludge meets the requirement of aggregate strength,others are 5.5% clay and 50.1% PFA. The burning temperature is the most important factor for the aggregate strength. The optimal sintering condition includes a furnace temperature of 471-490 ℃ when feeding,heating-up time of 10-11min from 500 to 1 000 ℃ ,the highest burning temperature between 1 161 and 1 170 ℃,retention time of 4 min at high burning temperature,and furnace temperature within 1 101-1 150 ℃ at burning end.展开更多
基金Project(CHENGKE2009-113) supported by Chongqing Municipal Administration Management Bureau
文摘The sintering conditions of artificial lightmass aggregate (LWA) made up of sewage sludge,clay and pulverized flyash (PFA) by trefoil rotary kiln were investigated. The influencing factors of the aggregate strength including furnace temperature when feeding,the heating-up time from 500 to 1 000 ℃ ,the highest burning temperature,retention time at the highest burning temperature and furnace temperature at burning end were analyzed by orthogonal tests. The results show that 44.4% (mass fraction) sewage sludge meets the requirement of aggregate strength,others are 5.5% clay and 50.1% PFA. The burning temperature is the most important factor for the aggregate strength. The optimal sintering condition includes a furnace temperature of 471-490 ℃ when feeding,heating-up time of 10-11min from 500 to 1 000 ℃ ,the highest burning temperature between 1 161 and 1 170 ℃,retention time of 4 min at high burning temperature,and furnace temperature within 1 101-1 150 ℃ at burning end.