With the development of aero-engine,gas import temperatures of hot section structural materials are increasingly higher.Metal alloy materials due to the rapidly decreased mechanical properties at relative high tempera...With the development of aero-engine,gas import temperatures of hot section structural materials are increasingly higher.Metal alloy materials due to the rapidly decreased mechanical properties at relative high temperature are gradually replaced with silicon-based non-oxide silicon carbide ceramics.However,silicon carbide ceramic materials tend to spall and deform in engine combustion environment,need environmental barrier coatings for the protection of the matrix.The preparation of Si/mullite/Yb2Si2O7 envir...展开更多
基金supported by the National Basic Research Program of China (2010CB934700)
文摘With the development of aero-engine,gas import temperatures of hot section structural materials are increasingly higher.Metal alloy materials due to the rapidly decreased mechanical properties at relative high temperature are gradually replaced with silicon-based non-oxide silicon carbide ceramics.However,silicon carbide ceramic materials tend to spall and deform in engine combustion environment,need environmental barrier coatings for the protection of the matrix.The preparation of Si/mullite/Yb2Si2O7 envir...