Growth of carbon nanotube arrays on various CtxMey alloy films by chemical vapour deposition method 被引量:2
1
作者 Pawel Mierczynski Sergey V.Dubkov +8 位作者 Sergey V.Bulyarskii Alexander A.Pavlov Sergey N.Skorik alexey yu trifonov Agnieszka Mierczynska Eugene P.Kitsyuk Sergey A.Gavrilov Tomasz P.Maniecki Dmitry G.Gromov 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2018年第3期472-480,共9页
Carbon nanotube (CNT) arrays were fabricated on Ct-Me-N-(O) alloys with content of Ct in the range of 6-40 at.% by chemical vapour deposition. The Ct was a catalytic metal from the group of the following elements... Carbon nanotube (CNT) arrays were fabricated on Ct-Me-N-(O) alloys with content of Ct in the range of 6-40 at.% by chemical vapour deposition. The Ct was a catalytic metal from the group of the following elements: Ni, Co, Fe, Pd, while Me was a transition metal from the group of IV-VII of the periodic table (where Me=Ti, V, Cr, Zr, Nb, Mo, Ta, W, Re). Carbon nanotubes were found to grow efficiently on the alloy surface with its composition containing Ti, V, Cr, Zr, Hf, Nb or Ta. The growth of CNTs was not observed when the alloy contained W or Re. Additions of oxygen and nitrogen in the alloy facilitated the formation of oxynitrides and catalyst extrusion on the alloy surface. Replacement of the metals in alloy composition affected the diameter of the resulting CNTs. The obtained results showed that the alloy films of varying thickness (10-500 nm) may be used for the CNTs growth. The resulting CNT material was highly homogenous and its synthesis reproducible. 展开更多
关键词 Carbon nanotubes Amorphous alloys Chemical vapour deposition Catalytic processes Thin films
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部