Vapor-phase transformations of furfural over SBA-15 silica supported Ni catalysts under H<sub>2</sub> in a continuous-flow reactor at atmospheric pressure and 170°C and 230°C were investiga...Vapor-phase transformations of furfural over SBA-15 silica supported Ni catalysts under H<sub>2</sub> in a continuous-flow reactor at atmospheric pressure and 170°C and 230°C were investigated. Two different samples having Ni loadings of 5 and 20 wt% (denoted here by SBA-5Ni and SBA-20Ni, respectively) were prepared by impregnation and characterized by atomic absorption spectroscopy, N<sub>2</sub> sorption analysis, X-ray diffraction, X-ray photoelectron spectroscopy, and transmission electron microscopy. Furan and furfuryl alcohol were two primary products resulting, respectively, from decarbonylation and hydrogenation of furfural. Under the conditions of the study, both reactions exhibited structure sensitivity evidenced by changes in product selectivities with variable Ni loadings. Compared with SBA-20Ni, the 5 wt% Ni catalyst showed better catalytic activity, reaching a furfural conversion of 100 mol% and a selectivity to furan of 98 mol%, after 5 h of time-on-stream at 230°C.展开更多
文摘Vapor-phase transformations of furfural over SBA-15 silica supported Ni catalysts under H<sub>2</sub> in a continuous-flow reactor at atmospheric pressure and 170°C and 230°C were investigated. Two different samples having Ni loadings of 5 and 20 wt% (denoted here by SBA-5Ni and SBA-20Ni, respectively) were prepared by impregnation and characterized by atomic absorption spectroscopy, N<sub>2</sub> sorption analysis, X-ray diffraction, X-ray photoelectron spectroscopy, and transmission electron microscopy. Furan and furfuryl alcohol were two primary products resulting, respectively, from decarbonylation and hydrogenation of furfural. Under the conditions of the study, both reactions exhibited structure sensitivity evidenced by changes in product selectivities with variable Ni loadings. Compared with SBA-20Ni, the 5 wt% Ni catalyst showed better catalytic activity, reaching a furfural conversion of 100 mol% and a selectivity to furan of 98 mol%, after 5 h of time-on-stream at 230°C.