目的:通过血清中白介素-17(IL-17)、胰岛素样生长因子-1(IGF-1)和可溶性细胞间粘附分子-1(ICAM-1)的水平表达及其相关性,对经^(131)I治疗的甲亢伴有甲状腺相关眼病患者的眼眶活动性进行评价。方法:88例Graves眼病(GO)患者依据临床活动... 目的:通过血清中白介素-17(IL-17)、胰岛素样生长因子-1(IGF-1)和可溶性细胞间粘附分子-1(ICAM-1)的水平表达及其相关性,对经^(131)I治疗的甲亢伴有甲状腺相关眼病患者的眼眶活动性进行评价。方法:88例Graves眼病(GO)患者依据临床活动性评分(CAS)标准分为GO活动期组(活动期组)52例、GO静止期组(静止期组)36例,另设Graves病无眼病组(无眼病组)34例和健康对照组(对照组)26例。采用酶联免疫吸附法测定血清IL-17、IGF-1、ICAM-1水平,同时测定血清游离三碘甲状原氨酸(FT_3)、游离甲状腺素(FT_4)、超敏促甲状腺素(sTSH)、促甲状腺素受体抗体(TRAb)水平。结果:经^(131)I治疗后,GO活动期组患者血清IL-17、IGF-1、ICAM-1水平明显高于健康对照组、静止期组和无眼病组(P<0.01);静止期组的血清IL-17水平高于健康对照组和无眼病组(P<0.05)。无眼病组的血清IL-17、IGF-1和ICAM-1水平与健康对照组比较,均无统计学差异(P> 0.05)。患者血清IL-17与ICAM-1、IGF-1的相关性分别为r=0.847、r=0.806(P<0.01);IGF-1与ICAM-1的相关性分别为r=0.882(P<0.01)。结论:Graves眼病患者经^(131)I治疗后血清IL-17、IGF-1、ICAM-1的表达水平明显高于静止期组。无眼病组及健康对照组,三个指标具有良好的相关性,对于GO眼病的病变进展监测和治疗效果观察具有一定的指导意义。 展开更多
关键词 GRAVES眼病 131I治疗 白介素-17 可溶性细胞间粘附分子-1 胰岛素样生长因子-1
下载PDF
Production of thick-walled hollow glass microspheres for inertial confinement fusion targets by sol-gel technology 被引量:6
2
作者 GAO Cong QI XiaoBo +4 位作者 WEI Sheng ZHANG ZhanWen LI Bo SHI Tao chu qiaomei 《Science China(Technological Sciences)》 SCIE EI CAS 2011年第9期2377-2385,共9页
To fabricate thick-walled hollow glass microspheres(HGMs)for inertial confinement fusion(ICF)targets by sol-gel technology,we investigated the effects of glass composition,blowing agent,refining temperature,pressure a... To fabricate thick-walled hollow glass microspheres(HGMs)for inertial confinement fusion(ICF)targets by sol-gel technology,we investigated the effects of glass composition,blowing agent,refining temperature,pressure and composition of furnace atmosphere on the wall thickness of HGMs by numerical simulation and experiments.The results showed that the residence times of the thick-walled HGMs in the encapsulating and refining phases decreased with the increase of wall thickness of HGMs.As a response to this challenge,glass composition must be optimized with the object of high surface tension and low viscosity at refining temperature,and the blowing agents with high decomposition temperature should be used,furthermore the concentration of blowing agents in gel particles must also be precisely controlled.The higher volume fraction of argon gas in the furnace atmosphere,the thicker the wall of HGMs.Due to the limited operating range of furnace atmosphere pressure,changing furnace atmosphere pressure could not significantly increase the wall thickness of HGMs.Although increasing refining temperature can improve the yield of high quality HGMs,a higher furnace atmosphere temperature may lead to a decrease in the wall thickness of HGMs.When the volume fraction of argon gas in the furnace atmosphere ranged from 80%to 95%,the furnace atmosphere pressure ranged from 1.0×105Pa to 1.25×105 Pa,and the refining temperature ranged from 1600°C to 1800°C,we produced thick-walled(5–10-m)HGMs with good sphericity,wall thickness uniformity and surface finish.However,the yield of high quality HGMs needs to be further improved.The compressive strength,tensile strength and permeation coefficient to deuterium gas of thick-walled HGMs at ambient temperature decreased with increase of the wall thickness. 展开更多
关键词 惯性约束聚变 空心玻璃微球 凝胶技术 厚壁 溶胶 生产 壁厚均匀性 HGMS