Enhanced strengthening by two-step progressive solution and aging treatment in AM50-4%(Zn,Y) magnesium alloy 被引量:1
1
作者 Shuai DAI Feng WANG +3 位作者 de-zhi ma Zhi WANG Zheng LIU Ping-li maO 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2018年第12期2419-2426,共8页
AM50-4%(Zn,Y)alloy with a Zn/Y mole ratio of6:1was subjected to thermal analysis,and the results were used for designing a two-step progressive solution treatment process.The effects of solution and aging treatments o... AM50-4%(Zn,Y)alloy with a Zn/Y mole ratio of6:1was subjected to thermal analysis,and the results were used for designing a two-step progressive solution treatment process.The effects of solution and aging treatments on the microstructure and mechanical properties of the AM50-4%(Zn,Y)alloy were investigated using OM,XRD,SEM/EDS,TEM,tensile test and hardness test.The experimental results demonstrated that the two-step progressive solution treatment could make theΦandβphases sufficiently dissolve into the matrix which possessed higher supersaturated degree of the dissolved solute compared with the one-step solution treatment.This resulted in a certain enhancement of the precipitation strengthening effect during the subsequent aging process.The precipitation of theФphase had a greater impact on the comprehensive mechanical properties of the alloy thanβphase precipitation when the aging treatment was performed at180℃.The peak aging strength of the AM50-4%(Zn,Y)alloy which was subjected to the two-step progressive solution treatment process(345℃for16h and375℃for6h)was obtained after the aging treatment at180℃for12h. 展开更多
关键词 AM50-4%(Zn Y) alloy thermal analysis solution aging treatment microstructure strengthening mechanism
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部