It is well known that the finer particle of cementing material has more pozzolanic reaction than the coarser. This paper investigates the shear properties of geocomposite soil with various particle sizes of bottom ash...It is well known that the finer particle of cementing material has more pozzolanic reaction than the coarser. This paper investigates the shear properties of geocomposite soil with various particle sizes of bottom ash. The geocomposite soil (GCS) in this study consists of dredged soil, bottom ash and cement for recycling dredged soil and bottom ash. Three different particle sizes of bottom ash passing No. 4 sieve, No. 40 sieve, and No. 140 sieve were added into soil mixtures, namely as GCS 4, GCS 40, and GCS 140, respectively. These bottom ashes have the same chemical component except for different particle sizes. Several mixtures were prepared with various contents of bottom ash ranging from 0 to 100% at 50% intervals by the weight of dry dredged soil. In this study, several series of unconfined compression test were carried out on the mixtures with various curing times. It is found that the unconfined compressive strength is a function of curing time and bottom ash content. For the curing time less than 28 days, the GCS 4 has higher unconfined compressive strength than the GCS 40 and GCS 140 due to the interlocking effect and friction between the particles with angular shape of coarse bottom ash. For the curing time larger than 28 days, the GCS 140 has higher strength due to the pozzolanic reaction. However, the ratios of secant modulus to unconfined compressive strength of three mixtures are almost the same, and in range of (46-100), regardless of mixing condition and curing time.展开更多
文摘It is well known that the finer particle of cementing material has more pozzolanic reaction than the coarser. This paper investigates the shear properties of geocomposite soil with various particle sizes of bottom ash. The geocomposite soil (GCS) in this study consists of dredged soil, bottom ash and cement for recycling dredged soil and bottom ash. Three different particle sizes of bottom ash passing No. 4 sieve, No. 40 sieve, and No. 140 sieve were added into soil mixtures, namely as GCS 4, GCS 40, and GCS 140, respectively. These bottom ashes have the same chemical component except for different particle sizes. Several mixtures were prepared with various contents of bottom ash ranging from 0 to 100% at 50% intervals by the weight of dry dredged soil. In this study, several series of unconfined compression test were carried out on the mixtures with various curing times. It is found that the unconfined compressive strength is a function of curing time and bottom ash content. For the curing time less than 28 days, the GCS 4 has higher unconfined compressive strength than the GCS 40 and GCS 140 due to the interlocking effect and friction between the particles with angular shape of coarse bottom ash. For the curing time larger than 28 days, the GCS 140 has higher strength due to the pozzolanic reaction. However, the ratios of secant modulus to unconfined compressive strength of three mixtures are almost the same, and in range of (46-100), regardless of mixing condition and curing time.