PREPARATION AND PROPERTIES OF HIGH STRENGTH RODS FROM L-AND D,L-LACTIDE COPOLYMER 被引量:2
1
作者 Yu-shan Hu Zheng-pu Zhang +2 位作者 Dong Song dong-ren bai Yong-mei Wang Institute of Polymer Chemistry State Key Laboratory of Functional Polymeric Materials for Adsorption and Separation, Nankai University Tianjin 300071, China 《Chinese Journal of Polymer Science》 SCIE CAS CSCD 2001年第4期351-357,共7页
Starling with the L- and D,L-lactide copolymer (L:DL = 9:1) [P(L-DL)LA] of M-W = 32.1 x 10(4), rods were obtained through a two stage process: (1) melt-extrusion at 155 degreesC, and (2) hot-drawing at 90 degreesC to ... Starling with the L- and D,L-lactide copolymer (L:DL = 9:1) [P(L-DL)LA] of M-W = 32.1 x 10(4), rods were obtained through a two stage process: (1) melt-extrusion at 155 degreesC, and (2) hot-drawing at 90 degreesC to various drawing ratios. The molecular weight of P(L-DL)LA fell to 9.3 x 10(4) as a consequence of the production process. The crystallization and molecular orientation of P(L-DL)LA developed as a result of the hot-drawing. The mechanical strengths of the rods increase with the drawing ratio; The maximum for tensile strength, bending strength, bending modulus, and shear strength are 329 MPa, 237 MPa, 8.8 GPa, and 157 MPa, respectively. 展开更多
关键词 P(L-DL)LA self-reinforcement ROD process bone fracture fixation
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部