Rolling Contact Fatigue Properties of SAE 8620 Steel after Case Carburizing 被引量:3
1
作者 Yan-guang CAO Le XU +2 位作者 gou-qiang zhang Jie SHI Mao-qiu WANG 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2016年第7期711-716,共6页
Rolling contact fatigue(RCF)properties of SAE 8620 steel after case carburizing have been investigated under two contact stresses of 4.0and 5.5GPa.Results show that the RCF life ranges from 2.5×10^6 to 3×1... Rolling contact fatigue(RCF)properties of SAE 8620 steel after case carburizing have been investigated under two contact stresses of 4.0and 5.5GPa.Results show that the RCF life ranges from 2.5×10^6 to 3×10^7 cycles under the contact stress of 5.5GPa,while it can be more than 1×10^8 cycles under the contact stress of 4.0GPa.The rated fatigue life L_(10)(lives with the 10%failure)is also drastically shortened from 9.8×10^6 to 5.4×10^5 cycles when the contact stress is increased from 4.0to 5.5GPa.Theoretical calculations and fractographs show that the maximum shear stress and the contact area increase with increasing the contact stress,making RCF tend to occur earlier. 展开更多
关键词 case hardening steel carburizing rolling contact fatigue contact stress SAE 8620steel
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部