In this work,we prepared SmCo/FeCo nanocomposite magnets with an enhanced magnetic performance by doping eutectic Sm-Ni alloy.The magnets without Sm-Ni alloy,with a grain size of 5-12 nm and an average size of~ 9 nm,a...In this work,we prepared SmCo/FeCo nanocomposite magnets with an enhanced magnetic performance by doping eutectic Sm-Ni alloy.The magnets without Sm-Ni alloy,with a grain size of 5-12 nm and an average size of~ 9 nm,are composed of Sm_(2)Co_(17) phase and FeCo phase,leading to a relatively low remanence of 0.0365A·m^(2)·g^(-1) and coercivity of 0.15 T,respectively.After doping 2.5 wt% Sm-Ni alloy,there is no obvious change on the grain size of SmCo/FeCo magnets.展开更多
基金financially supported by the National Natural Science Foundation of China (No.51701066)。
文摘In this work,we prepared SmCo/FeCo nanocomposite magnets with an enhanced magnetic performance by doping eutectic Sm-Ni alloy.The magnets without Sm-Ni alloy,with a grain size of 5-12 nm and an average size of~ 9 nm,are composed of Sm_(2)Co_(17) phase and FeCo phase,leading to a relatively low remanence of 0.0365A·m^(2)·g^(-1) and coercivity of 0.15 T,respectively.After doping 2.5 wt% Sm-Ni alloy,there is no obvious change on the grain size of SmCo/FeCo magnets.