Effects of annealing temperature and neodymium concentration on structural and photoluminescence properties of Nd^(3+)-doped Y_(2)O_(3)-SiO_(2) powders 被引量:2
1
作者 NoSoung Myoung gyeong bok jung 《Journal of Rare Earths》 SCIE EI CAS CSCD 2021年第6期651-656,I0002,共7页
We report the structural and photoluminescence(PL) properties of Nd^(3+)-doped Y_(2)O_(3)-SiO_(2) powders(Y_(2)O_(3)-SiO_(2):Nd^(3+)) as functions of annealing temperature and Nd^(3+) ion doping concentration.Y_(2)O_(... We report the structural and photoluminescence(PL) properties of Nd^(3+)-doped Y_(2)O_(3)-SiO_(2) powders(Y_(2)O_(3)-SiO_(2):Nd^(3+)) as functions of annealing temperature and Nd^(3+) ion doping concentration.Y_(2)O_(3)-SiO_(2):Nd^(3+)powders were prepared using the high-energy ball-milling(HEBM) method,and their structural and PL properties were investigated using X-ray diffraction(XRD),Fourier transform infrared(FTIR) spectroscopy,and PL spectroscopy.The XRD results reveal a cubic phase without impurities,and the peak broadening decreases with an increase in annealing temperature due to the increase in the crystallite size.The PL emission intensity increases with an increase in annealing temperature.The highest PL emission intensity is observed for the 300-min milled mixture annealed at 1000℃ for 1 h with a Nd^(3+) concentration of 1 mol%.The PL peaks excited by 800 nm radiation were detected,centered at 1080 nm(^(4)F_(3/2)→^(4)I_(11/2)) and 1350 nm(^(4)F_(3/2)→^(4)I_(13/2)). 展开更多
关键词 Nd^(3+)-doped Y_(2)O_(3)-SiO_(2)powders High-energy ball-milling method Near infrared photoluminescence emission Rare earth Annealing temperature
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部