Fabrication and analysis of TIG welding-brazing butt joints of in-situ TiB2/7050 composite and TA2
1
作者 Huan-huan Sun Yi-bo Ren +4 位作者 Yang Feng hao-qiang ba Dong Chen Chun-juan Xia Hao-wei Wang 《Defence Technology(防务技术)》 SCIE EI CAS CSCD 2021年第3期1062-1070,共9页
Lightweight hybrid structures of Al MMCs and titanium alloy dissimilar materials have great prospect in the defence industry application. So, it is necessary to join Al MMCs with Ti metal to achieve this structural de... Lightweight hybrid structures of Al MMCs and titanium alloy dissimilar materials have great prospect in the defence industry application. So, it is necessary to join Al MMCs with Ti metal to achieve this structural design. In this work, in-situ Ti B_(2)/7050 composite and TA2 were firstly attempted to join by TIG welding-brazing technique. The result was that the intact welding-brazing butt joint was successfully fabricated. The joint presents dual characteristics, being a brazing on TA2 side and a welding on Ti B_(2)/7050 side. At brazing joint side, ER4043 filler metal effectively wets on TA2 under TIG heating condition,and a continuous interfacial reaction layer with 1 e3 mm is formed at welded metal/TA2 interface. The whole interfacial reaction layers are composed of Ti(Al Si)3 intermetallic compounds(IMCs), but their morphologies at the different regions present obvious distinguishes. The microhardness of the reaction layers is as much as 141 e190 HV. At welding joints side, the fusion zone appears the equixaed crystal structure, and the grain sizes are much smaller than those of welded metal, which is attributed to the effect of Ti B2 particulates from the melted Ti B_(2)/7050 on acceleration formation and inhibiting growth for the new crystal nucleus. The tensile test results show that average tensile strength of the optimal welding-brazing joint is able to achieve 138 MPa. The failure of the tensile joint occurs by quasi-cleavage pattern, and the cracks initiate from the IMCs layer at the groove surface of TA2 and propagate into the welded metal. 展开更多
关键词 In-situ TiB2/7050 composite TA2 TIG welding-brazing FABRICATION Analysis
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部