Owing to its low cost,short process and low energy consumption,semi-solid processing(SSP)of aluminum(Al)and magnesium(Mg)alloys has been considered as a competitive approach to fabricate complicated components with ex...Owing to its low cost,short process and low energy consumption,semi-solid processing(SSP)of aluminum(Al)and magnesium(Mg)alloys has been considered as a competitive approach to fabricate complicated components with excellent performance.Over the past decade,significant progress has been achieved in deeply understanding the SSP process,the microstructure and performance of the fabricated components in China.This paper starts with a retrospective overview of some common slurry preparation methods,followed by presenting the performance and the underlying mechanisms of SSP fabricated alloys.Then,the mainstream opinions on the microstructure evolution and rheological flow behavior of semi-solid slurry are discussed.Subsequently,the general situation and some recent examples of industrial applications of SSP are presented.Finally,special attention is paid to the unresolved issues and the future directions in SSP of Al and Mg alloys in China.展开更多
In the present study,numerical simulation method was used to analyze the conditions,resulting in the formation of blisters during solution heat treatment.Blister formation is considered to occur as the height of blist...In the present study,numerical simulation method was used to analyze the conditions,resulting in the formation of blisters during solution heat treatment.Blister formation is considered to occur as the height of blister reaches 5μm.The effects of process parameters on the magnitude of the forming temperatures of blister(Tb)were discussed.Two kinds of Al-Si alloys were used to analyze the effect of mechanical properties of the alloys on blister forming conditions.Simulation results show that decreasing the initial pressure in gas hole,the long-short axial ratio of gas hole and the size of gas hole,as well as increasing the depth of gas hole and the strength of alloy are helpful to increase the critical temperature of forming blister.These conclusions are helpful for casters to understand the conditions controlling blister formation during solution heat treatment and take actions to avoid the blister defects.展开更多
基金financial supports from the Shenzhen Science and Technology Innovation Commission, China (Nos. KQTD20170328154443162, JCYJ20180305123432756)。
文摘Owing to its low cost,short process and low energy consumption,semi-solid processing(SSP)of aluminum(Al)and magnesium(Mg)alloys has been considered as a competitive approach to fabricate complicated components with excellent performance.Over the past decade,significant progress has been achieved in deeply understanding the SSP process,the microstructure and performance of the fabricated components in China.This paper starts with a retrospective overview of some common slurry preparation methods,followed by presenting the performance and the underlying mechanisms of SSP fabricated alloys.Then,the mainstream opinions on the microstructure evolution and rheological flow behavior of semi-solid slurry are discussed.Subsequently,the general situation and some recent examples of industrial applications of SSP are presented.Finally,special attention is paid to the unresolved issues and the future directions in SSP of Al and Mg alloys in China.
基金financially supported by the National Key Research and Development Program of China (No.2016YFB0301003)Shenzhen Science and Technology Innovation Commission under Projects (Nos.JCYJ20170307110223452,KQJSCX20170328155402991 and KQTD20170328154443162)。
文摘In the present study,numerical simulation method was used to analyze the conditions,resulting in the formation of blisters during solution heat treatment.Blister formation is considered to occur as the height of blister reaches 5μm.The effects of process parameters on the magnitude of the forming temperatures of blister(Tb)were discussed.Two kinds of Al-Si alloys were used to analyze the effect of mechanical properties of the alloys on blister forming conditions.Simulation results show that decreasing the initial pressure in gas hole,the long-short axial ratio of gas hole and the size of gas hole,as well as increasing the depth of gas hole and the strength of alloy are helpful to increase the critical temperature of forming blister.These conclusions are helpful for casters to understand the conditions controlling blister formation during solution heat treatment and take actions to avoid the blister defects.