In this paper,overcharge behaviors and thermal runaway(TR)features of large format lithium-ion(Liion)cells with different cathode materials(LiFePO4(LFP),Li[Ni_(1/3)Co_(1/3)Mn_(1/3)]O_(2)(NCM111),Li[Ni_(0.6)Co_(0.2)Mn_...In this paper,overcharge behaviors and thermal runaway(TR)features of large format lithium-ion(Liion)cells with different cathode materials(LiFePO4(LFP),Li[Ni_(1/3)Co_(1/3)Mn_(1/3)]O_(2)(NCM111),Li[Ni_(0.6)Co_(0.2)Mn_(0.2)]O_(2)(NCM622)and Li[Ni_(0.8)Co_(0.1)Mn_(0.1)]O_(2)(NCM811))were investigated.The results showed that,under the same overcharge condition,the TR of LFP Li-ion cell occurred earlier compared with the NCM Li-ion cells,indicating its poor overcharge tolerance and high TR risk.However,when TR occurred,LFP Li-ion cell exhibited lower maximum temperature and mild TR response.All NCM Liion cells caught fire or exploded during TR,while the LFP Li-ion cell only released a large amount of smoke without fire.According to the overcharge behaviors and TR features,a safety assessment score system was proposed to evaluate the safety of the cells.In short,NCM Li-ion cells have better performance in energy density and overcharge tolerance(or low TR risk),while LFP Li-ion cell showed less severe response to overcharging(or less TR hazards).For NCM Li-ion cells,as the ratio of nickel in cathode material increases,the thermal stability of the cathode materials becomes poorer,and the TR hazards increase.Such a comparison study on large format Li-ion cells with different cathode materials can provide deeper insights into the overcharge behaviors and TR features,and provide guidance for engineers to reasonably choose battery materials in automotive applications.展开更多
Large-format lithium-ion(Li-ion) batteries with high energy density for electric vehicles are prone to thermal runaway(or even explosion) under abusive conditions. In this study, overcharge induced explosion behaviors...Large-format lithium-ion(Li-ion) batteries with high energy density for electric vehicles are prone to thermal runaway(or even explosion) under abusive conditions. In this study, overcharge induced explosion behaviors of large-format Li-ion pouch cells with Li[NiCoMn]Ocathode at different current rates(C-rates)(0.5C, 1C, 2C) were investigated. The explosion characteristics of the cells were elucidated by discussing the evolution of the cell voltage, the surface temperature and the shock wave pressure.Generally, the whole overcharge process could be divided into four stages according to the evolution of several key parameters and the overcharge behaviors;the overcharge C-rate has a great influence on cells’ thermal behaviors. The experimental results showed that the thermal runaway process of Liion cells caused by overcharging consisted of two kinds of explosions, physical explosion and chemical explosion. The existence of observable negative pressure zone in the pressure curves indicated that the Li-ion cells are not a self-supplying oxygen system during the explosion. Further, the explosion dynamics parameters were matched. An explosion TNT-equivalent conversion strategy that depended on the pressure of the shock wave was utilized to evaluate the released energy and its hazards. In addition, with respect to the overcharge of Li-ion pouch cells, a safety assessment method and a safety management method were proposed based on the explosion behaviors. From the perspective of battery safety, this study is of great significance for the safety design of Li-ion cells and can provide guidance for engineers to optimize the safety function of battery packs.展开更多
基金supported by the National Natural Science Foundation of China(Nos.U1564206,U1764258)the National Key R&D Program of China(No.2018YFB0105700)+1 种基金the support from China Scholarship Council(No.201806030115)supported by the Department of Energy(DOE),Office of Electricity(OE)at Oak Ridge National Laboratory managed by UL-Battelle LLC under contract DE-AC05-00OR22725。
文摘In this paper,overcharge behaviors and thermal runaway(TR)features of large format lithium-ion(Liion)cells with different cathode materials(LiFePO4(LFP),Li[Ni_(1/3)Co_(1/3)Mn_(1/3)]O_(2)(NCM111),Li[Ni_(0.6)Co_(0.2)Mn_(0.2)]O_(2)(NCM622)and Li[Ni_(0.8)Co_(0.1)Mn_(0.1)]O_(2)(NCM811))were investigated.The results showed that,under the same overcharge condition,the TR of LFP Li-ion cell occurred earlier compared with the NCM Li-ion cells,indicating its poor overcharge tolerance and high TR risk.However,when TR occurred,LFP Li-ion cell exhibited lower maximum temperature and mild TR response.All NCM Liion cells caught fire or exploded during TR,while the LFP Li-ion cell only released a large amount of smoke without fire.According to the overcharge behaviors and TR features,a safety assessment score system was proposed to evaluate the safety of the cells.In short,NCM Li-ion cells have better performance in energy density and overcharge tolerance(or low TR risk),while LFP Li-ion cell showed less severe response to overcharging(or less TR hazards).For NCM Li-ion cells,as the ratio of nickel in cathode material increases,the thermal stability of the cathode materials becomes poorer,and the TR hazards increase.Such a comparison study on large format Li-ion cells with different cathode materials can provide deeper insights into the overcharge behaviors and TR features,and provide guidance for engineers to reasonably choose battery materials in automotive applications.
基金sponsored by the China Postdoctoral Science Foundation(China National Postdoctoral Program for Innovative Talents,BX2021036)the National Natural Science Foundation of China(52072040,U21A20170)supported by the Department of Energy(DOE),Office of Electricity(OE)at Oak Ridge National Laboratory managed by UL-Battelle LLC(DE-AC0500OR22725)。
文摘Large-format lithium-ion(Li-ion) batteries with high energy density for electric vehicles are prone to thermal runaway(or even explosion) under abusive conditions. In this study, overcharge induced explosion behaviors of large-format Li-ion pouch cells with Li[NiCoMn]Ocathode at different current rates(C-rates)(0.5C, 1C, 2C) were investigated. The explosion characteristics of the cells were elucidated by discussing the evolution of the cell voltage, the surface temperature and the shock wave pressure.Generally, the whole overcharge process could be divided into four stages according to the evolution of several key parameters and the overcharge behaviors;the overcharge C-rate has a great influence on cells’ thermal behaviors. The experimental results showed that the thermal runaway process of Liion cells caused by overcharging consisted of two kinds of explosions, physical explosion and chemical explosion. The existence of observable negative pressure zone in the pressure curves indicated that the Li-ion cells are not a self-supplying oxygen system during the explosion. Further, the explosion dynamics parameters were matched. An explosion TNT-equivalent conversion strategy that depended on the pressure of the shock wave was utilized to evaluate the released energy and its hazards. In addition, with respect to the overcharge of Li-ion pouch cells, a safety assessment method and a safety management method were proposed based on the explosion behaviors. From the perspective of battery safety, this study is of great significance for the safety design of Li-ion cells and can provide guidance for engineers to optimize the safety function of battery packs.