Thermal Oxidative Degradation and Ageing Performance of Silicone Rubber Filled with Attapulgite 被引量:2
1
作者 hua-hua zhao Huan-ling Song +3 位作者 Xin-yao Tao Ge-xin Chen Ai-qin Wang Ling-jun Chou 《Chinese Journal of Chemical Physics》 SCIE CAS CSCD 2021年第3期309-322,I0048,共15页
The natural attapulgite(NAPT)was disaggregated by high-pressure homogenization technology combined with extrusion process to prepare the attapulgite with disaggregated rod crystal bundles(DAPT)and large specific surfa... The natural attapulgite(NAPT)was disaggregated by high-pressure homogenization technology combined with extrusion process to prepare the attapulgite with disaggregated rod crystal bundles(DAPT)and large specific surface area of 133.7 m^(2)/g.NAPT and DAPT were incorporated into the silicone rubber to obtain the composite NAPTSR and DAPT-SR by mechanical blending method,respectively.After thermal oxidative ageing at 300℃ for 0.5 h,temperature for the 5%weight loss increased greatly from 385℃ of the neat silicone rubber to 396-399℃ with addition of NAPT and DAPT.NAPT and DAPT enhanced the interaction between the filler nanoparticles and rubber matrix thus inhibited the nanoparticle agglomeration.The conservation rate of the side methyl group in NAPT-SR and DAPT-SR was greatly improved after ageing.Therefore,the thermal oxidative degradation and ageing performance of the silicone rubber composites was significantly reinforced.Moreover,DAPT could greatly restrain the growth of nanoparticles after ageing.Therefore,DAPT-SR showed the better retention of tensile strength(40.6%),elongation at break(34.9%)and tear strength(30.1%)compared with the corresponding mechanical properties of the neat silicone rubber(10.6%,7.4%,and 5.0%)after ageing. 展开更多
关键词 Silicone rubber ATTAPULGITE COMPOSITES Thermal oxidative degradation Ageing
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部