In this study,indium oxide(In2O3) thin-film transistors(TFTs) are fabricated by two kinds of low temperature solution-processed technologies(Ta ≤ 300℃),i.e.,water-based(DIW-based) process and alkoxide-based...In this study,indium oxide(In2O3) thin-film transistors(TFTs) are fabricated by two kinds of low temperature solution-processed technologies(Ta ≤ 300℃),i.e.,water-based(DIW-based) process and alkoxide-based(2-ME-based)process.The thickness values,crystallization properties,chemical structures,surface roughness values,and optical properties of In2O3 thin-films and the electrical characteristics of In2O3 TFTs are studied at different annealing temperatures.Thermal annealing at higher temperature leads to an increase in the saturation mobility(μsat) and a negative shift in the threshold voltage(VTH).The DIW-based processed In2O3-TFT annealed at 300℃ exhibits excellent device performance,and one annealed at 200℃ exhibits an acceptable μsat of 0.86 cm^2/V·s comparable to that of a-Si:H TFTs,whereas the 2-ME-based TFT annealed at 300℃ exhibits an abundant μsat of 1.65 cm^2/Vs and one annealed at 200℃ is inactive.The results are attributed to the fact that the DIW-based process induces a higher degree of oxidation and less defect states than the 2-ME-based process at the same temperature.The DIW-based process for fabricating the In2O3 TFT opens the way for the development of nontoxic,low-cost,and low-temperature oxide electronics.展开更多
基金Project supported by the National Natural Science Foundation of China(Grant No.61675024)the National Basic Research Program of China(Grant No.2014CB643600)
文摘In this study,indium oxide(In2O3) thin-film transistors(TFTs) are fabricated by two kinds of low temperature solution-processed technologies(Ta ≤ 300℃),i.e.,water-based(DIW-based) process and alkoxide-based(2-ME-based)process.The thickness values,crystallization properties,chemical structures,surface roughness values,and optical properties of In2O3 thin-films and the electrical characteristics of In2O3 TFTs are studied at different annealing temperatures.Thermal annealing at higher temperature leads to an increase in the saturation mobility(μsat) and a negative shift in the threshold voltage(VTH).The DIW-based processed In2O3-TFT annealed at 300℃ exhibits excellent device performance,and one annealed at 200℃ exhibits an acceptable μsat of 0.86 cm^2/V·s comparable to that of a-Si:H TFTs,whereas the 2-ME-based TFT annealed at 300℃ exhibits an abundant μsat of 1.65 cm^2/Vs and one annealed at 200℃ is inactive.The results are attributed to the fact that the DIW-based process induces a higher degree of oxidation and less defect states than the 2-ME-based process at the same temperature.The DIW-based process for fabricating the In2O3 TFT opens the way for the development of nontoxic,low-cost,and low-temperature oxide electronics.