An aromatic diamine monomer,4,4'-bis(3-amino-5-trifluoromethyl phenoxy)-biphenyl (TFBPDA),wassynthesized via the nucleophilic displacement reaction of 3,5-dinitrobenzotrifluoride and 4,4'-biphenol.The monomer ...An aromatic diamine monomer,4,4'-bis(3-amino-5-trifluoromethyl phenoxy)-biphenyl (TFBPDA),wassynthesized via the nucleophilic displacement reaction of 3,5-dinitrobenzotrifluoride and 4,4'-biphenol.The monomer wasreacted with various aromatic dianhydrides via the high temperature polycondensation procedure to provide a series ofpolyimides.The polyimides,PI-1 to PI-4,show good solubility not only in aprotic solvents,such as N-methyl-2-pyrrolidinone and N,N-dimethylacetamide,but also in many common solvents,such as m-cresol,chloroform andcyclopentanone.PI-4,derived from 4,4'-(hexafluoroisopropylidene)diphthalic anhydride and TFBPDA,was even soluble intoluene.Moreover,PI films exhibit good thermal stability,outstanding transparency in the visible light region and acceptablemechanical and electrical properties.The excellent combined properties of the polyimides make them as a good candidate forfabricating microelectronics.展开更多
Organo-soluble fluorinated polyimides were synthesized by the polycondensation of a new aromatic diamine α,α-bis(4-amino-3,5-dimethylphenyl)-4'-fluorophenyl methane with several aromatic dianhydrides.The one-ste...Organo-soluble fluorinated polyimides were synthesized by the polycondensation of a new aromatic diamine α,α-bis(4-amino-3,5-dimethylphenyl)-4'-fluorophenyl methane with several aromatic dianhydrides.The one-step polymerizationprocedure was conducted at 180℃ in m-cresol,producing the polyimides with inherent viscosities of 0.68-0.76 dL.g^(-1).Thepolyimides could be soluble not only in polar aprotic solvents,such as N-methyl-2-pyrrolidinone,and N,N-dimethylacetamide,but also in common organic solvents,such as chloroform,cyclopentanone,m-cresol and so on.Thepolyimide films show excellent transparency with the UV-Vis cut-off lengths of 310-360 nm and light transmittances ofhigher than 80% in the visible region.In addition,the polyimides exhibit good thermal stability with an initial decompositiontemperature(T_d)higher than 530℃ and have more than 60% of residual weight retentions at 700℃.展开更多
基金This project is supported by the National Natural Science Foundation of China(NSFC)for distinguished Young Scholars(No.59925310).
文摘An aromatic diamine monomer,4,4'-bis(3-amino-5-trifluoromethyl phenoxy)-biphenyl (TFBPDA),wassynthesized via the nucleophilic displacement reaction of 3,5-dinitrobenzotrifluoride and 4,4'-biphenol.The monomer wasreacted with various aromatic dianhydrides via the high temperature polycondensation procedure to provide a series ofpolyimides.The polyimides,PI-1 to PI-4,show good solubility not only in aprotic solvents,such as N-methyl-2-pyrrolidinone and N,N-dimethylacetamide,but also in many common solvents,such as m-cresol,chloroform andcyclopentanone.PI-4,derived from 4,4'-(hexafluoroisopropylidene)diphthalic anhydride and TFBPDA,was even soluble intoluene.Moreover,PI films exhibit good thermal stability,outstanding transparency in the visible light region and acceptablemechanical and electrical properties.The excellent combined properties of the polyimides make them as a good candidate forfabricating microelectronics.
基金This work was supported by the National Natural Science Foundation of China(NSFC)for distinguished Young Scholars(No.59925310).
文摘Organo-soluble fluorinated polyimides were synthesized by the polycondensation of a new aromatic diamine α,α-bis(4-amino-3,5-dimethylphenyl)-4'-fluorophenyl methane with several aromatic dianhydrides.The one-step polymerizationprocedure was conducted at 180℃ in m-cresol,producing the polyimides with inherent viscosities of 0.68-0.76 dL.g^(-1).Thepolyimides could be soluble not only in polar aprotic solvents,such as N-methyl-2-pyrrolidinone,and N,N-dimethylacetamide,but also in common organic solvents,such as chloroform,cyclopentanone,m-cresol and so on.Thepolyimide films show excellent transparency with the UV-Vis cut-off lengths of 310-360 nm and light transmittances ofhigher than 80% in the visible region.In addition,the polyimides exhibit good thermal stability with an initial decompositiontemperature(T_d)higher than 530℃ and have more than 60% of residual weight retentions at 700℃.