To expand the use of metal–organic frameworks(MOFs)based self-lubricating composite,flexible MOFs MIL-88D has been studied as a nanocontainer for loading lubricant.In this work,the mechanism of oleamine adsorption an...To expand the use of metal–organic frameworks(MOFs)based self-lubricating composite,flexible MOFs MIL-88D has been studied as a nanocontainer for loading lubricant.In this work,the mechanism of oleamine adsorption and desorption by MIL-88D was investigated through molecular simulations and experiments.Molecular simulations showed that the oleamines can be physically adsorbed into open MIL-88Ds with the Fe and O atoms of MIL-88D interacting with oleamine NH2-group.Higher temperature can cause Ole@MIL-88D to release more oleamines,while higher pressure on Ole@MIL-88D caused less oleamines released.Moreover the Ole@MIL-88D was incorporated into epoxy resin(EP)for friction tests.The optimum mass ratio of MIL-88D to EP is 15 wt%,and the EP/Ole@MIL-88D prefers light load and high frequency friction.This work suggests that flexible MOFs can be used as a nanocontainer for loading lubricant,and can be used as a new self-lubricating composite.展开更多
基金Foundation of State Key Laboratory of Tribology in Advanced Equipment at Tsinghua University(Grant No.SKLTKF21B13)Natural Science Foundation of Hebei Province of China(Grant No.E2021203092)National Natural Science Foundation of China(Grant No.51905297)are acknowledged.
文摘To expand the use of metal–organic frameworks(MOFs)based self-lubricating composite,flexible MOFs MIL-88D has been studied as a nanocontainer for loading lubricant.In this work,the mechanism of oleamine adsorption and desorption by MIL-88D was investigated through molecular simulations and experiments.Molecular simulations showed that the oleamines can be physically adsorbed into open MIL-88Ds with the Fe and O atoms of MIL-88D interacting with oleamine NH2-group.Higher temperature can cause Ole@MIL-88D to release more oleamines,while higher pressure on Ole@MIL-88D caused less oleamines released.Moreover the Ole@MIL-88D was incorporated into epoxy resin(EP)for friction tests.The optimum mass ratio of MIL-88D to EP is 15 wt%,and the EP/Ole@MIL-88D prefers light load and high frequency friction.This work suggests that flexible MOFs can be used as a nanocontainer for loading lubricant,and can be used as a new self-lubricating composite.