Targeted heat treatment of additively manufactured Ti-6Al-4V for controlled formation of Bi-lamellar microstructures 被引量:1
1
作者 Cecilie V.Funch Alessandro Palmas +6 位作者 Kinga Somlo Emilie H.Valente Xiaowei Cheng konstantinos poulios Matteo Villa Marcel A.J.Somers Thomas L.Christiansena 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2021年第22期67-76,共10页
Laser powder bed fusion(L-PBF)was utilized to produce specimens in Ti-6Al-4V,which were subjected to a bi-lamellar heat treatment,which produces microstructures consisting of primary α-lamellae and a fine secondary ... Laser powder bed fusion(L-PBF)was utilized to produce specimens in Ti-6Al-4V,which were subjected to a bi-lamellar heat treatment,which produces microstructures consisting of primary α-lamellae and a fine secondary α-phase inside the inter-lamellar β-regions.The bi-lamellar microstructure was obtained as(i)a direct bi-lamellar heat treatment from the asbuilt condition or(ii)a bi-lamellar heat treatment preceded by a β-homogenization.For the bi-lamellar treatment with β-homogenization,cooling rates in the range 1-500 K/min were applied after homogenization in β-region followed by inter-critical annealing in the α+β region at various temperatures in the range 850-950℃.The microstructures were characterized using various microscopical techniques.Mechanical testing with Vickers hardness indentation and tensile testing was performed.The bi-lamellar microstructure was harder when compared to a soft fully lamellar microstructure,because of the presence of fine α-platelets inside the β-lamellae.Final low temperature ageing provided an additional hardness increase by precipitation hardening of the primary α-regions.The age hardened bi-lamellar microstructure shows a similar hardness as the very fine,as-built martensitic microstructure.The bi-lamellar microstructure has more favorable mechanical properties than the as-built condition,which has high strength,but poor ductility.After the bi-lamellar heat treatment,the elongation was improved by more than 250%.Due to the very high strength of the as-built condition,loss of tensile strength is unavoidable,resulting in a reduction of tensile strength of~18%. 展开更多
关键词 Additive manufacturing TI-6AL-4V Targeted heat treatment Bi-lamellar microstructures Laser powder bed fusion
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部