富钇混合稀土对AM60镁合金显微组织与力学性能的影响 被引量:5
1
作者 田政 张德平 +6 位作者 王鸿燕 杜海 唐定骧 孟健 l.l.rokhlin T.V.Dobatkina F.M.Elkin 《中国稀土学报》 CAS CSCD 北大核心 2008年第6期729-733,共5页
在AM60镁合金的基础上添加不同质量分数的富Y混合稀土(分别为0.5%,1.0%,1.5%,2.0%),研究了富钇混合稀土对AM60镁合金显微组织与力学性能的影响。结果表明:富Y稀土的加入使AM60镁合金的显微组织明显细化,并能显著提高合金的抗拉强度、屈... 在AM60镁合金的基础上添加不同质量分数的富Y混合稀土(分别为0.5%,1.0%,1.5%,2.0%),研究了富钇混合稀土对AM60镁合金显微组织与力学性能的影响。结果表明:富Y稀土的加入使AM60镁合金的显微组织明显细化,并能显著提高合金的抗拉强度、屈服强度及延伸率。加入混合稀土后,合金中形成块状的铝钇化合物Al2Y,Al6Mn6Y,β-Mg17Al12相数量减少。当稀土加入量为1%时,合金的各方面性能达到最好。 展开更多
关键词 镁合金 显微组织 力学性能 AM60 稀土
下载PDF
Effect of multiaxial deformation on structure, mechanical properties, and corrosion resistance of a Mg-Ca alloy 被引量:1
2
作者 N.Yu.Yurchenko N.D.Stepanov +7 位作者 G.A.Salishchev V.N.Serebryany N.S.Martynenko E.A.Lukyanova l.l.rokhlin N.Birbilis S.V.Dobatkin Y.Z.Estrin 《Journal of Magnesium and Alloys》 SCIE EI CAS CSCD 2022年第1期284-298,共15页
This article provides a report on the effect of multiaxial deformation(MAD) on the structure, texture, mechanical characteristics, and corrosion resistance of the Mg-0.8(wt.)% Ca alloy. MAD was carried out on the allo... This article provides a report on the effect of multiaxial deformation(MAD) on the structure, texture, mechanical characteristics, and corrosion resistance of the Mg-0.8(wt.)% Ca alloy. MAD was carried out on the alloy in the as-cast and the annealed states in multiple passes, with a stepwise decrease in the deformation temperature from 450 to 250 ℃ in 50 ℃ steps. The cumulative true strain at the end of the process was 22.5. In the case of the as-cast alloy, this resulted in a refined microstructure characterized by an average grain size of 2.7 μm and a fraction of high-angle boundaries(HABs) of 57.6%. The corresponding values for the annealed alloy were 2.1 μm and 68.2%. The predominant mechanism of structure formation was associated with discontinuous and continuous dynamic recrystallization acting in concert. MAD was also shown to lead to the formation of a rather sharp prismatic texture in the as-cast alloy, whilst in the case of the annealed one the texture was weakened. A displacement of the basal poles {00.4} from the periphery to the center of a pole figure was observed. These changes in the microstructure and texture gave rise to a significant improvement of the mechanical characteristics of the alloy. This included an increase of the ultimate tensile strength reaching 308 MPa for annealed material and 264 MPa for the as-cast one in conjunction with a twofold increase in ductility. A further important result of the MAD processing was a reduction of the rate of electrochemical corrosion, as indicated by a significant decrease in the corrosion current density in both microstructural states of the alloy studied. 展开更多
关键词 Metals and alloys Multiaxial deformation MICROSTRUCTURE RECRYSTALLIZATION Mechanical properties CORROSION
下载PDF
铈镧混合稀土对AZ91D压铸镁合金显微组织和蠕变性能的影响 被引量:18
3
作者 张德平 田政 +3 位作者 唐定骧 孟健 l.l.rokhlin T.V.Dobatkina 《稀有金属》 EI CAS CSCD 北大核心 2010年第2期202-209,共8页
研究了不同含量Ce/La(x=0,0.1,0.5,1.0)对AZ91D镁合金显微组织及蠕变性能的影响。通过X射线衍射(XRD)、金相显微镜(OM)、扫描电镜(SEM)及能谱分析(EDX)观察与分析表明,压铸AZ91D镁合金中添加Ce/La后,除了α-Mg,β-Mg17Al12相之外,还生... 研究了不同含量Ce/La(x=0,0.1,0.5,1.0)对AZ91D镁合金显微组织及蠕变性能的影响。通过X射线衍射(XRD)、金相显微镜(OM)、扫描电镜(SEM)及能谱分析(EDX)观察与分析表明,压铸AZ91D镁合金中添加Ce/La后,除了α-Mg,β-Mg17Al12相之外,还生成了新的稀土化合物Al11RE3(RE=Ce/La)化合物,并且细化了合金显微组织、提高了合金室温和高温力学性能。生成的Al11RE3(RE=Ce/La)高温热稳定相使AZ91D+xCe/La(x=0,0.1,0.5,1.0)合金在150℃,50MPa下的蠕变抗力优于AZ91D镁合金,1%Ce/La的合金与AZ91D相比,蠕变延伸率低了0.2%,最小蠕变速率从2.30×10-8s-1降低到2.02×10-8s-1。蠕变试样的微观组织结构分析表明:AZ91D合金的蠕变机制主要以晶界滑移方式为主,Al11RE3(RE=Ce/La)热稳定相在晶界处延缓和阻碍了晶界断裂的过程。 展开更多
关键词 AZ91D镁合金 晶粒细化 抗蠕变性能 显微组织 铈镧混合稀土