Non-alcoholic fatty liver disease(NAFLD)is the most common liver disease in Asia.Several studies have shown that NAFLD is associated with obesity,insulin resistance,type 2 diabetes,hypertension,hyperlipidemia,and meta... Non-alcoholic fatty liver disease(NAFLD)is the most common liver disease in Asia.Several studies have shown that NAFLD is associated with obesity,insulin resistance,type 2 diabetes,hypertension,hyperlipidemia,and metabolic syndrome(MS)[1].Several studies concluded that indicators such as body mass index(BMI),waist circumference(WC)。 展开更多
关键词 NAFLD PROBABILITY LIVER
下载PDF
高炉冶金矿渣特性及其在ZTA陶瓷烧结中的作用
2
作者 卢红霞 高凯 +1 位作者 李明亮 梁新星 《矿产保护与利用》 2020年第3期26-33,共8页
高炉渣是由炼铁高炉产生的一种工业废渣,其中含有CaO、Al2O3、SiO2等硅酸盐成分和少量Fe2O3、TiO2、ZrO2等析晶形核剂。高炉渣在855℃热处理1 h,可形核析出1μm左右的Ca2Al2SiO7微晶,这表明高炉渣具有较高的析晶活性。向ZTA中添加质量... 高炉渣是由炼铁高炉产生的一种工业废渣,其中含有CaO、Al2O3、SiO2等硅酸盐成分和少量Fe2O3、TiO2、ZrO2等析晶形核剂。高炉渣在855℃热处理1 h,可形核析出1μm左右的Ca2Al2SiO7微晶,这表明高炉渣具有较高的析晶活性。向ZTA中添加质量分数为4%的高炉渣,1550℃烧结30 min,低温下ZTA陶瓷的力学性能明显提升,抗弯强度和断裂韧性分别为650 MPa和6.03 MPa·m^1/2,比相同温度下未添加高炉渣时分别提高了15%和14.2%,烧结温度降低了50℃以上。颗粒细化的高炉渣掺入ZTA陶瓷基体,烧结过程中高炉渣产生的液相促进了Al2O3棒晶的生长,受力过程中棒晶的拔出和裂纹的偏转有利于ZTA陶瓷力学性能的提升;高炉渣在高温下的析晶增强了ZTA陶瓷的晶界强度,进一步提高了材料的力学性能。 展开更多