Application Study on β-Sialon-AI_2O_3 Brick in Iron Ladle
1
作者 liuxiongzhang HEShengping 《China's Refractories》 CAS 2003年第1期23-27,共5页
The microstructure and slag erosion fractal dimension of reaction interface of β-Sialon-Al2O3 brick used in 300 Mt iron ladle of Baosteel have been studied by SEM and XRD. The results indicated that β-Sialon-Al2O3 b... The microstructure and slag erosion fractal dimension of reaction interface of β-Sialon-Al2O3 brick used in 300 Mt iron ladle of Baosteel have been studied by SEM and XRD. The results indicated that β-Sialon-Al2O3 brick exhibited excellent slag resistance. The main wear mechanism of β-Sialon-Al2O3 brick is mainly from the spalling caused by thermal mechanical stress and attacked by slag secondly. 展开更多
关键词 β-Sialon-Al2O3 brick Iron ladle Microstruc-ture Wear mechanism