A subbituminous coal was oxidized with air at 150℃on a fixed bed for 4 h and xanthated with carbondisulfide in a basic solution,at 30 or 5-10℃.This xanthated coal was evaluated for the removal of Hg^(2+)and Cd^(2+)f...A subbituminous coal was oxidized with air at 150℃on a fixed bed for 4 h and xanthated with carbondisulfide in a basic solution,at 30 or 5-10℃.This xanthated coal was evaluated for the removal of Hg^(2+)and Cd^(2+)from 7,000 mg/L aqueous solutions;metal concentrations were detemmined by atomic absorption spectrometry.The ionexchange of the xanthated coal was compared against those of the original subbituminous coal,a sulfonated subbituminouscoal,activated carbon,commercial activated carbon,and commercial synthetic resin.The commercial synthetic resinshowed the highest exchange capacity(concentration factor 98%)followed by the xanthated coal(concentration factor 96%).The retention of cadmium on the sulfonated subbituminous coal was lower(exchange capacity 0.56 meq/g)thanthat of xanthated coals(1.85±0.09 meq/g).Our xanthated coal showed a better Cd^(2+)removal(8l%o against 15%)than anon preoxidized 40-h-xanthated coal,which shows that oxidation of coal increased the amount of oxygenated groups whichenhanced xanthation.展开更多
文摘A subbituminous coal was oxidized with air at 150℃on a fixed bed for 4 h and xanthated with carbondisulfide in a basic solution,at 30 or 5-10℃.This xanthated coal was evaluated for the removal of Hg^(2+)and Cd^(2+)from 7,000 mg/L aqueous solutions;metal concentrations were detemmined by atomic absorption spectrometry.The ionexchange of the xanthated coal was compared against those of the original subbituminous coal,a sulfonated subbituminouscoal,activated carbon,commercial activated carbon,and commercial synthetic resin.The commercial synthetic resinshowed the highest exchange capacity(concentration factor 98%)followed by the xanthated coal(concentration factor 96%).The retention of cadmium on the sulfonated subbituminous coal was lower(exchange capacity 0.56 meq/g)thanthat of xanthated coals(1.85±0.09 meq/g).Our xanthated coal showed a better Cd^(2+)removal(8l%o against 15%)than anon preoxidized 40-h-xanthated coal,which shows that oxidation of coal increased the amount of oxygenated groups whichenhanced xanthation.