A liquid-solid fluidized bed separator, used for the separation of coarse slime, was developed. Test parti- cles sized in the range from 0.25 to 0.5, 0.5 to 1.0, and 0.25 to 1.0 mm were separated in the liquid-solid f...A liquid-solid fluidized bed separator, used for the separation of coarse slime, was developed. Test parti- cles sized in the range from 0.25 to 0.5, 0.5 to 1.0, and 0.25 to 1.0 mm were separated in the liquid-solid fluidized bed. Beds with column heights of 1200, 1500, and 1800 mm were tried. The clean coal and the railings were subsequently analyzed by float-sink testing. The results showed that the ash and yield of clean coal both decreased with increasing column height, for all three size fractions, and that the ash of the clean coal obtained from tests on the broader size fraction was less than that from the narrower sized fractions. The separation density decreased with increasing column height. The lowest E value was seen for a column height of 1500 ram, for which conditions the separation density was 1.45 g/cm3. The E value was 0.084 for the 0.25-0.5 mm fraction but the corresponding separation density was 1.48 g/cm3, and the E value 0.089, for the broader 0.25-1.0 mm fraction.展开更多
基金supports for this work provided by the National Natural Science Foundation of China (No. 50974120)the Fundamental Research Funds for the Central Universities (No.2010QNB08)
文摘A liquid-solid fluidized bed separator, used for the separation of coarse slime, was developed. Test parti- cles sized in the range from 0.25 to 0.5, 0.5 to 1.0, and 0.25 to 1.0 mm were separated in the liquid-solid fluidized bed. Beds with column heights of 1200, 1500, and 1800 mm were tried. The clean coal and the railings were subsequently analyzed by float-sink testing. The results showed that the ash and yield of clean coal both decreased with increasing column height, for all three size fractions, and that the ash of the clean coal obtained from tests on the broader size fraction was less than that from the narrower sized fractions. The separation density decreased with increasing column height. The lowest E value was seen for a column height of 1500 ram, for which conditions the separation density was 1.45 g/cm3. The E value was 0.084 for the 0.25-0.5 mm fraction but the corresponding separation density was 1.48 g/cm3, and the E value 0.089, for the broader 0.25-1.0 mm fraction.