LaNiO3 was synthesized by sol-gel method in which lanthanum nitrate and nickel nitrate were used as start materials and citric acid was used as complex for gel formation.The precursor was dried and subsequently heated...LaNiO3 was synthesized by sol-gel method in which lanthanum nitrate and nickel nitrate were used as start materials and citric acid was used as complex for gel formation.The precursor was dried and subsequently heated at elevated temperature to form the desired product.XRD analysis shows that pure LaNiO3 was synthesized.Electrical conductivity and electrochemical performance of the material were tested.The electrical conductivity decreases from 34.5that there are current peaks in the curve, which is the evidence of the electrochemical activity of LaNiO3.展开更多
文摘LaNiO3 was synthesized by sol-gel method in which lanthanum nitrate and nickel nitrate were used as start materials and citric acid was used as complex for gel formation.The precursor was dried and subsequently heated at elevated temperature to form the desired product.XRD analysis shows that pure LaNiO3 was synthesized.Electrical conductivity and electrochemical performance of the material were tested.The electrical conductivity decreases from 34.5that there are current peaks in the curve, which is the evidence of the electrochemical activity of LaNiO3.