Pt-(Sn,Re)/HZSM5-HMS catalysts were evaluated for n-heptane isomerization at 200–350 ℃.To characterize the catalyst,X-ray diffraction,X-ray fluorescene,Fourier transform infrared spectroscopy,ultraviolet-visible d...Pt-(Sn,Re)/HZSM5-HMS catalysts were evaluated for n-heptane isomerization at 200–350 ℃.To characterize the catalyst,X-ray diffraction,X-ray fluorescene,Fourier transform infrared spectroscopy,ultraviolet-visible diffuse reflectance spectroscopy,temperature-programmed reduction of H2,temperature-programmed desorption of NH3,infrared spectroscopy of adsorbed pyridine,H2 chemisorption,nitrogen adsorption-desorption,scanning electron microscopy and thermogravimetric analysis were performed.Kinetics of n-C7 isomerization were investigated under various hydrogen and n-C7 pressures,and the effects of reaction conditions on catalytic performance were studied.The results showed that bi-and trimetallic catalysts exhibit better performance than monometallic catalysts for this reaction.For example,a maximum i-C7 selectivity( 〉74%) and multibranched isomer selectivity(40%) were observed for Pt-Sn/HZSM5-HMS at 200 ℃.展开更多
文摘Pt-(Sn,Re)/HZSM5-HMS catalysts were evaluated for n-heptane isomerization at 200–350 ℃.To characterize the catalyst,X-ray diffraction,X-ray fluorescene,Fourier transform infrared spectroscopy,ultraviolet-visible diffuse reflectance spectroscopy,temperature-programmed reduction of H2,temperature-programmed desorption of NH3,infrared spectroscopy of adsorbed pyridine,H2 chemisorption,nitrogen adsorption-desorption,scanning electron microscopy and thermogravimetric analysis were performed.Kinetics of n-C7 isomerization were investigated under various hydrogen and n-C7 pressures,and the effects of reaction conditions on catalytic performance were studied.The results showed that bi-and trimetallic catalysts exhibit better performance than monometallic catalysts for this reaction.For example,a maximum i-C7 selectivity( 〉74%) and multibranched isomer selectivity(40%) were observed for Pt-Sn/HZSM5-HMS at 200 ℃.