A review of refractory high-entropy alloys 被引量:5
1
作者 Yu-sheng TIAN Wen-zhe ZHOU +6 位作者 Qing-biao TAN ming-xu wu Shen QIAO Guo-liang ZHU An-ping DONG Da SHU Bao-de SUN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第11期3487-3515,共29页
This work reviews recent progress in the alloy design,microstructure,and mechanical properties of refractory high-entropy alloys(RHEAs).What’s more,the underlying strengthening mechanisms and deformation behavior are... This work reviews recent progress in the alloy design,microstructure,and mechanical properties of refractory high-entropy alloys(RHEAs).What’s more,the underlying strengthening mechanisms and deformation behavior are discussed.Composed mainly of near-equimolar refractory elements,RHEAs have superior mechanical properties,especially at high temperatures.However,many of them have limited room-temperature ductility.Much work has been done to solve this trade-off,and some of the RHEAs have the potential to be used for high-temperature applications in the future.In addition to their mechanical properties,RHEAs have other attractive properties,such as biocompatibility and wear resistance,which are discussed.Finally,current problems and future suggestions for RHEAs are discussed. 展开更多
关键词 refractory high-entropy alloys MICROSTRUCTURE high-temperature strength mechanical properties dislocations
下载PDF
Effect of trace boron on grain refinement of commercially pure aluminum by Al-5Ti-1B 被引量:2
2
作者 Fei XIAO ming-xu wu +8 位作者 Yi-xiao WANG Wen-zhe ZHOU Shu-bin WANG Dong-hong WANG Guo-liang ZHU Michael JIANG Da SHU Jia-wei MI Bao-de SUN 《Transactions of Nonferrous Metals Society of China》 SCIE EI CAS CSCD 2022年第4期1061-1069,共9页
The effect of boron content on grain refinement of commercially pure aluminum by Al-5Ti-1B was quantitatively assessed.When the boron content is less than 0.03 wt.%,the refining performance of Al-5Ti-1B gradually is w... The effect of boron content on grain refinement of commercially pure aluminum by Al-5Ti-1B was quantitatively assessed.When the boron content is less than 0.03 wt.%,the refining performance of Al-5Ti-1B gradually is weakened as the boron content increases,which is attributed to the reaction of boron with the Al_(3)Ti interlayer on TiB_(2)and the consumption of solute Ti.On the contrary,when the boron content exceeds 0.03 wt.%,the refining performance of Al-5Ti-1B gradually recovers with increasing boron content,which is related to the formation of primary AlB_(2)particles that provide additional nucleant substrates. 展开更多
关键词 aluminum alloy casting Al-5Ti-1B grain refinement boron treatment NUCLEATION
下载PDF