A fully characterised natural rubber latex was subjected to mechanical degradation by stirring at intervals. The resistance to oxidative degradation of the different samples were studied by measuring the Plasticity r...A fully characterised natural rubber latex was subjected to mechanical degradation by stirring at intervals. The resistance to oxidative degradation of the different samples were studied by measuring the Plasticity retention indices (PRI). The results show that there is an enhancement of the PRI from 57% for the undegraded rubber to 79% for the one-hour degraded sample. Further degradation resulted in decrease of PRI as time of degradation increased. Therefore, the one-hour degraded sample is a special rubber with high oxidation resistance which is of great importance in engineering. (Author abstract) 9 Refs.展开更多
文摘A fully characterised natural rubber latex was subjected to mechanical degradation by stirring at intervals. The resistance to oxidative degradation of the different samples were studied by measuring the Plasticity retention indices (PRI). The results show that there is an enhancement of the PRI from 57% for the undegraded rubber to 79% for the one-hour degraded sample. Further degradation resulted in decrease of PRI as time of degradation increased. Therefore, the one-hour degraded sample is a special rubber with high oxidation resistance which is of great importance in engineering. (Author abstract) 9 Refs.