作者 Kahtan S. Mohammed Baba Gowon +2 位作者 Shamsul Baharin Bin Jamaluddin Zuhailawati Hussain polycarp evarastics 《Open Journal of Metal》 2015年第3期27-36,共10页
Fabrication of full-density W-brass composites is very difficult to achieve because of evaporation of zinc, insolubility of W and brass and compacts expansion. In this study, to achieve full-density W-brass composites... Fabrication of full-density W-brass composites is very difficult to achieve because of evaporation of zinc, insolubility of W and brass and compacts expansion. In this study, to achieve full-density W-brass composites, mechanical alloying (MA) and activated sintering process were utilized. Mechanical coating of W with Ni using high energy planetary ball mill was carried out. The milling was divided into two stages: to alloy and modify the surface of W with Ni for enhanced activation. The microstructure of the milled powders and sintered compacts, elemental composition and phases present were studied by using scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX) and X-ray diffraction (XRD) respectively. As-received powder compacts was also sintered under the same condition for comparison purpose. The effects of milling time on the microstructure, sinterability and the hardness of the composites were investigated. It was observed that the samples produced from 8 h milled powder had the highest relative sintered density (98% TD) and microhardness (234 Hv). On the other hand, the samples from the as-received powders expanded and had a relative sintered density of (67% TD) and microhardness as low as 24 Hv. The significance of this study is the possibility of producing W-brass composites as a cheaper alternative to W-Cu composites. 展开更多
关键词 W-Brass Mechanical ALLOYING Microstructure Expansion HARDNESS
下载PDF
The Effects of Sintering Temperature on the Densification of Mechanically Alloyed W-Brass Composites
2
作者 Baba Gowon Kahtan S. Mohammed +2 位作者 Shamsul Baharin Bin Jamaluddin Zuhailawati Hussain polycarp evarastics 《Open Journal of Metal》 2015年第3期19-26,共8页
Prealloyed (PA) and premixed (PM) W-brass with the composition of 60 wt% W, 1 wt% Ni and 39 wt% brass was sintered at the temperature of 800&degC, 920&degC and 1000&degC each. As a result of difficulties i... Prealloyed (PA) and premixed (PM) W-brass with the composition of 60 wt% W, 1 wt% Ni and 39 wt% brass was sintered at the temperature of 800&degC, 920&degC and 1000&degC each. As a result of difficulties in the densification of W-Cu and W-Cu alloys, mechanical alloying (MA) and activated sintering were combined. The powders were mechanically alloyed for 13 hours to produce nanosized W grains embedded in brass. The microstructure and properties of these composites with increase in sintering temperature has been studied. Both prealloyed and premixed composites sintered at 800&degC (solid state sintering) and 920&degC (sub-solidus state sintering) have lower sintered densities and hardness. The densification rate in the premixed composites was observed to be higher than that of the prealloyed composites. Their densification and properties increased with the increase in the sintering temperature. Premixed composite sintered at 1000&degC had 91.0% sintered density, 180 Hv microhardness against 76.0% and 133 Hv respectively for prealloyed composite at the same temperature. The values of electrical conductivity in both prealloyed and premixed composites increased with increase in temperature. 展开更多
关键词 W-Brass TEMPERATURE DENSIFICATION Prealloy HARDNESS