Study on heat treatment blister of squeeze casting parts
1
作者 TONG Wen-jun qi Lin qi pi-xiang 《China Foundry》 SCIE CAS 2007年第2期108-111,共4页
Heat treatment blister is one of the common defects found in squeeze casting parts, which is related to squeeze mode, process and mold. For direct squeeze-casting parts, solution heat treatment can be performed smooth... Heat treatment blister is one of the common defects found in squeeze casting parts, which is related to squeeze mode, process and mold. For direct squeeze-casting parts, solution heat treatment can be performed smoothly as long as oil-based paint is not used and air exhaust is well arranged. For indirect squeeze casting parts, solution heat treatment can also be applied when additional factors are taken into consideration, including well designed internal feeding system and strictly controlled liquid metal filling velocity to prevent from inclusions. 展开更多
关键词 squeeze casting DEFECTS heat treatment