Solid-State Reaction and Vacancy-Type Defects in Bilayer Fe/Hf Studied by the Slow Positron Beam
1
作者 K. Yamada T. Sasaki +5 位作者 T. Nagata I. Kanazawa r. suzuki T. Ohdaira K. Nozawa F. Komori 《Journal of Applied Mathematics and Physics》 2015年第2期233-239,共7页
The positron annihilation lifetimes and the Doppler broadening by slow positron beam are measured in thin Fe films with thickness 500 nm, a thin Hf film with thickness 100 nm, and the bilayer Fe (50 nm)/Hf (50 nm) on ... The positron annihilation lifetimes and the Doppler broadening by slow positron beam are measured in thin Fe films with thickness 500 nm, a thin Hf film with thickness 100 nm, and the bilayer Fe (50 nm)/Hf (50 nm) on quartz glass substrate. We have analyzed the behavior in vacancy-type defects in each layer through some deposition temperatures and annealing. It is observed that the thin Fe film, the thin Hf film, and the bilayer Fe (50 nm)/Hf (50 nm) already contain many vacancy-type defects. We have investigated the change of densities of the vacancy-carbon complex and the small vacancy-cluster with carbons, through solid-state amorphization of Fe (50 nm)/Hf (50 nm) bilayer. 展开更多
关键词 Metallic Films POSITRON ANNIHILATION Measurement SOLID-STATE Reaction FE Film Diffusion Vacancy-Type Defects
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部