The effects of carbon addition (0.01wt%-0.43wt%) on a Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-1Nd (wt%) alloy with a bimodal microstructure were investigated. Electron probe microanalysis was carried out to examine the partitio...The effects of carbon addition (0.01wt%-0.43wt%) on a Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-1Nd (wt%) alloy with a bimodal microstructure were investigated. Electron probe microanalysis was carried out to examine the partitioning behavior of carbon and the relation of carbon content to the distributions of Al and Mo in the primary αp phase (α p) and β transformed structure (β). It was found that interstitial carbon is enriched in the α p phase and its content slightly reduces with the increase of the volume fraction of α p. The measurements of carbon content in the present alloy with an α p of 15vol% showed that the carbon content in the α p phase increases with the increment of carbon addition until a maximum but keeps almost constant in the β phase. The addition of carbon reduces the solubility of Al and Mo in the α p phase and leads to the increment of Mo partitioning to the β phase. When the carbon content is over 0.17wt% (0.67at%), carbide precipitation occurs in the matrix and its volume fraction is related to the volume fraction of α p which can be explained in term of the difference of carbon solubility in the α p and β phases.展开更多
The mechanical behavior and the effect of pre-strain on recovery behavior of Ti50Ni47Fe3 (at. pct) alloy were investigated systematically by tensile and recovered tests accompanied by electrical resistance measurement...The mechanical behavior and the effect of pre-strain on recovery behavior of Ti50Ni47Fe3 (at. pct) alloy were investigated systematically by tensile and recovered tests accompanied by electrical resistance measurement. Ti50Ni47Fe3 alloy has different deformation behaviors at different temperature ranges, the deformation curves in different temperature range can be classified into four kinds. The start temperature of recovery increases with the increase of pre-strain. There exists an optimal deformation condition, at which the specimen exhibits maximum free recovery strain. With increasing pre-strain the recovery stress increases and reaches the maximum at 8% pre-strain. R-phase to parent transition offered about 0.2% recovery strain. With pre-strain increasing the recovery stress increases and reaches to the maximum at 8% pre-strain. The recovery stress is corresponding with the critical stress of stress-induced martensitic transformation.展开更多
文摘The effects of carbon addition (0.01wt%-0.43wt%) on a Ti-5.6Al-4.8Sn-2Zr-1Mo-0.35Si-1Nd (wt%) alloy with a bimodal microstructure were investigated. Electron probe microanalysis was carried out to examine the partitioning behavior of carbon and the relation of carbon content to the distributions of Al and Mo in the primary αp phase (α p) and β transformed structure (β). It was found that interstitial carbon is enriched in the α p phase and its content slightly reduces with the increase of the volume fraction of α p. The measurements of carbon content in the present alloy with an α p of 15vol% showed that the carbon content in the α p phase increases with the increment of carbon addition until a maximum but keeps almost constant in the β phase. The addition of carbon reduces the solubility of Al and Mo in the α p phase and leads to the increment of Mo partitioning to the β phase. When the carbon content is over 0.17wt% (0.67at%), carbide precipitation occurs in the matrix and its volume fraction is related to the volume fraction of α p which can be explained in term of the difference of carbon solubility in the α p and β phases.
文摘The mechanical behavior and the effect of pre-strain on recovery behavior of Ti50Ni47Fe3 (at. pct) alloy were investigated systematically by tensile and recovered tests accompanied by electrical resistance measurement. Ti50Ni47Fe3 alloy has different deformation behaviors at different temperature ranges, the deformation curves in different temperature range can be classified into four kinds. The start temperature of recovery increases with the increase of pre-strain. There exists an optimal deformation condition, at which the specimen exhibits maximum free recovery strain. With increasing pre-strain the recovery stress increases and reaches the maximum at 8% pre-strain. R-phase to parent transition offered about 0.2% recovery strain. With pre-strain increasing the recovery stress increases and reaches to the maximum at 8% pre-strain. The recovery stress is corresponding with the critical stress of stress-induced martensitic transformation.