In this study nanoporous NiO was prepared using Ni(CH3COO)2,4H2O, folic acid and water as starting material, template and solvent respectively, by sol gel method followed by calcination at 400℃. The solid product was...In this study nanoporous NiO was prepared using Ni(CH3COO)2,4H2O, folic acid and water as starting material, template and solvent respectively, by sol gel method followed by calcination at 400℃. The solid product was characterized by X-ray diffraction (XRD), nitrogen adsorption-desorption, scanning electron microscopy (SEM), transmission electron microscopy (TEM) Fourier transform infrared (FT-IR) and photoluminescence (PL) techniques. The particle size of the nanoparticles estimated by XRD was in good agreement with the particle size obtained by TEM analysis (4-5nm). It was also found that the prepared nanoporous NiO show very good activity for photodegredation of dye organic pollutants such as Congo red (91%) during 1.5 hours.展开更多
文摘In this study nanoporous NiO was prepared using Ni(CH3COO)2,4H2O, folic acid and water as starting material, template and solvent respectively, by sol gel method followed by calcination at 400℃. The solid product was characterized by X-ray diffraction (XRD), nitrogen adsorption-desorption, scanning electron microscopy (SEM), transmission electron microscopy (TEM) Fourier transform infrared (FT-IR) and photoluminescence (PL) techniques. The particle size of the nanoparticles estimated by XRD was in good agreement with the particle size obtained by TEM analysis (4-5nm). It was also found that the prepared nanoporous NiO show very good activity for photodegredation of dye organic pollutants such as Congo red (91%) during 1.5 hours.