Surface flashover of spacers is a key factor limiting the application of HVDC GIS/GIL,while the charge accumula-tion on the surface of the spacer could have a potential adverse effect on the surface flashover voltage....Surface flashover of spacers is a key factor limiting the application of HVDC GIS/GIL,while the charge accumula-tion on the surface of the spacer could have a potential adverse effect on the surface flashover voltage.This paper discusses the laws regarding distribution patterns of surface charges and the related mechanisms.The field-dependent property is discussed in detail to comprehensively illustrate the charge transport mecha-nism and explain the research differences regarding different surface charge patterns obtained by previous researchers.In addition,the main surface charge control methods for epoxy resin are summarized and discussed.The potential research directions of charge control methods and key points in manufacturing of spacers used in HVDC GIS/GIL are also explored.展开更多
Surface charge accumulation on the spacers is one of the key issues restraining the development of HVDC GIS/GIL.The precise measurement of surface charge properties provides the basis for further study of the surface ...Surface charge accumulation on the spacers is one of the key issues restraining the development of HVDC GIS/GIL.The precise measurement of surface charge properties provides the basis for further study of the surface charge transport mechanism as well as the charge-induced flashover mechanism under DC voltage.In this study,the authors discuss their perspective on the current status,development needs and potential developing orientation of surface charge characterisation techniques.Different surface potential measurement methods and charge inversion algorithms are reviewed regarding the previous studies and future research needs.Drawbacks and outlooks of surface charge measurement techniques are also discussed with the background of laboratory experiment results and on-site measurements.It is hopefully that this study can serve as a useful guide reference for researchers within the same research field.More importantly,it is authors’hope that this study can inspire some novel ideas for readers into developing of more accurate and scientific interface charge characterisation techniques.展开更多
To investigate the effect of fluorination on surface electrical performance of ethylene propylene rubber(EPR),four pieces of EPR specimens are prepared and fluorinated for different duration ranging from 120 min to 48...To investigate the effect of fluorination on surface electrical performance of ethylene propylene rubber(EPR),four pieces of EPR specimens are prepared and fluorinated for different duration ranging from 120 min to 480 min.The surface morphology and element compositions of experimental specimens are tested.The surface potential decay and complex permittivity are measured.The tracking discharge property and the erosion properties after tracking test are investigated.The surface charge transport and electrical property tailoring mechanism are discussed.The results show that when the fluorination duration is from 120 min to 360 min,the surface morphology gradually becomes flat and compact with time,and the surface resistance to electrical tracking is improved.While an excessive fluorination with the duration of 480 min leads to a significant increase in surface conductivity and a weakening in the resistance to electrical tracking,which is mainly due to a change in surface morphology.The recommended fluorination duration for an optimised surface property is between 240 and 360 min for EPR specimen.展开更多
The evolution of properties of crosslinked polyethylene(XLPE)-based insulating mate-rials under radio-chemical ageing conditions is presented and discussed.In total,seven different polymer compounds were tested,charac...The evolution of properties of crosslinked polyethylene(XLPE)-based insulating mate-rials under radio-chemical ageing conditions is presented and discussed.In total,seven different polymer compounds were tested,characterised by an increasing quantity of additives,for example,antioxidants(AOs)and fillers as flame retardants.Samples were analysed using different testing techniques,that is,Fourier Transform Infra-Red and dielectric spectroscopy.This allowed a broad characterisation of the polymer,bringing to good correlations between the arising of new chemical groups caused by ageing and the modifications on the complex permittivity.Phenol-based AOs are found to be the most efficient in terms of protection against oxidation.On the contrary,flame retardants are concluded not to have any impact on the material ageing.Acquired data were then treated using the principal component analysis.The data treatment successfully distinguished the material composition(with and without additives)and the ageing environments.The results confirm the relevance of this analysis in understanding the impact of irradiation on the chemical and functional properties of the polymer materials studied.展开更多
During operation of high voltage(HV)motors,different types of discharges,e.g.surface discharge,corona discharge and bar-to-bar discharge can occur at the same time,increasing the difficulty of partial discharge(PD)sou...During operation of high voltage(HV)motors,different types of discharges,e.g.surface discharge,corona discharge and bar-to-bar discharge can occur at the same time,increasing the difficulty of partial discharge(PD)sources determination and PDs pattern identification.In this study,the end-winding of a 10 kV motor coil was artificially aged and the related PD was measured.The initiation and variation of different PDs under multi-factor stresses were studied.The localised fingerprints coexisting with multiple PDs were identified and analysed.The results confirm that the end-winding discharge process was significantly influenced by the experiment relative humidity(RH)and temperature.The bar-to-bar discharge was easily recognised at a lower voltage since the identification of bar-to-bar discharge pattern would be affected by the corona discharge pattern at a higher voltage.It is shown that it is more difficult for the corona discharge to be detected when RH exceeded 80%,while the surface discharge dominated at the higher RH.In addition,the PDs were more easily identified with the rise of the temperature.This study can provide a reference in PD identification test and be useful for the PD online monitoring of HV motors.展开更多
基金This study is financially supported by the National Basic Research Program(2017YFB0903800)and the Electric Power Research Institute,Yunnan Electric Power Grid Co.Ltd,Kunming,Yunnan 650217,China(YNKJXM20160146).
文摘Surface flashover of spacers is a key factor limiting the application of HVDC GIS/GIL,while the charge accumula-tion on the surface of the spacer could have a potential adverse effect on the surface flashover voltage.This paper discusses the laws regarding distribution patterns of surface charges and the related mechanisms.The field-dependent property is discussed in detail to comprehensively illustrate the charge transport mecha-nism and explain the research differences regarding different surface charge patterns obtained by previous researchers.In addition,the main surface charge control methods for epoxy resin are summarized and discussed.The potential research directions of charge control methods and key points in manufacturing of spacers used in HVDC GIS/GIL are also explored.
基金the National Natural Science Foundation of China(Grant No.51677113).
文摘Surface charge accumulation on the spacers is one of the key issues restraining the development of HVDC GIS/GIL.The precise measurement of surface charge properties provides the basis for further study of the surface charge transport mechanism as well as the charge-induced flashover mechanism under DC voltage.In this study,the authors discuss their perspective on the current status,development needs and potential developing orientation of surface charge characterisation techniques.Different surface potential measurement methods and charge inversion algorithms are reviewed regarding the previous studies and future research needs.Drawbacks and outlooks of surface charge measurement techniques are also discussed with the background of laboratory experiment results and on-site measurements.It is hopefully that this study can serve as a useful guide reference for researchers within the same research field.More importantly,it is authors’hope that this study can inspire some novel ideas for readers into developing of more accurate and scientific interface charge characterisation techniques.
基金This study is financially supported by National Natural Science Foundation of China(51577123,51807060 and 51737005).
文摘To investigate the effect of fluorination on surface electrical performance of ethylene propylene rubber(EPR),four pieces of EPR specimens are prepared and fluorinated for different duration ranging from 120 min to 480 min.The surface morphology and element compositions of experimental specimens are tested.The surface potential decay and complex permittivity are measured.The tracking discharge property and the erosion properties after tracking test are investigated.The surface charge transport and electrical property tailoring mechanism are discussed.The results show that when the fluorination duration is from 120 min to 360 min,the surface morphology gradually becomes flat and compact with time,and the surface resistance to electrical tracking is improved.While an excessive fluorination with the duration of 480 min leads to a significant increase in surface conductivity and a weakening in the resistance to electrical tracking,which is mainly due to a change in surface morphology.The recommended fluorination duration for an optimised surface property is between 240 and 360 min for EPR specimen.
文摘The evolution of properties of crosslinked polyethylene(XLPE)-based insulating mate-rials under radio-chemical ageing conditions is presented and discussed.In total,seven different polymer compounds were tested,characterised by an increasing quantity of additives,for example,antioxidants(AOs)and fillers as flame retardants.Samples were analysed using different testing techniques,that is,Fourier Transform Infra-Red and dielectric spectroscopy.This allowed a broad characterisation of the polymer,bringing to good correlations between the arising of new chemical groups caused by ageing and the modifications on the complex permittivity.Phenol-based AOs are found to be the most efficient in terms of protection against oxidation.On the contrary,flame retardants are concluded not to have any impact on the material ageing.Acquired data were then treated using the principal component analysis.The data treatment successfully distinguished the material composition(with and without additives)and the ageing environments.The results confirm the relevance of this analysis in understanding the impact of irradiation on the chemical and functional properties of the polymer materials studied.
基金The authors wish to express their deepest gratitude to the financial supports of the State National Natural Science Foundation(Nos.51377113,51577123 and U1510112)which ensured the successful completion of the experiment.
文摘During operation of high voltage(HV)motors,different types of discharges,e.g.surface discharge,corona discharge and bar-to-bar discharge can occur at the same time,increasing the difficulty of partial discharge(PD)sources determination and PDs pattern identification.In this study,the end-winding of a 10 kV motor coil was artificially aged and the related PD was measured.The initiation and variation of different PDs under multi-factor stresses were studied.The localised fingerprints coexisting with multiple PDs were identified and analysed.The results confirm that the end-winding discharge process was significantly influenced by the experiment relative humidity(RH)and temperature.The bar-to-bar discharge was easily recognised at a lower voltage since the identification of bar-to-bar discharge pattern would be affected by the corona discharge pattern at a higher voltage.It is shown that it is more difficult for the corona discharge to be detected when RH exceeded 80%,while the surface discharge dominated at the higher RH.In addition,the PDs were more easily identified with the rise of the temperature.This study can provide a reference in PD identification test and be useful for the PD online monitoring of HV motors.