We conducted a series of experimental studies on the metallurgical properties of N-lump and F-lump ores used in Baosteel’s blast furnace, including thermal cracking, low-temperature reduction pulverization, reducibil...We conducted a series of experimental studies on the metallurgical properties of N-lump and F-lump ores used in Baosteel’s blast furnace, including thermal cracking, low-temperature reduction pulverization, reducibility, and droplet properties.The results show that the thermal burst properties of N-lump ore are better than those of F-lump ore.The low-temperature reduction degradation index(RDI) pulverization of the charge is the best when the ratios of N-lump ore and F-lump ore account for 35% each.The reduction performance of the charge is improved when F-lump and N-lump ores are mixed with sinter.In the softening-melting performance experiment, when the proportion of N-lump ore is 40%,the characteristic area value(S) as the charge permeability index is the smallest.When F-lump ore is mixed with sinter, its droplet performance improves compared with that of single F-lump ore.The proportion of F-lump ore should not exceed 15%.展开更多
文摘We conducted a series of experimental studies on the metallurgical properties of N-lump and F-lump ores used in Baosteel’s blast furnace, including thermal cracking, low-temperature reduction pulverization, reducibility, and droplet properties.The results show that the thermal burst properties of N-lump ore are better than those of F-lump ore.The low-temperature reduction degradation index(RDI) pulverization of the charge is the best when the ratios of N-lump ore and F-lump ore account for 35% each.The reduction performance of the charge is improved when F-lump and N-lump ores are mixed with sinter.In the softening-melting performance experiment, when the proportion of N-lump ore is 40%,the characteristic area value(S) as the charge permeability index is the smallest.When F-lump ore is mixed with sinter, its droplet performance improves compared with that of single F-lump ore.The proportion of F-lump ore should not exceed 15%.