Nanoscale tungsten powder was prepared by reducing nanoscale tungsten trioxide in hydrogen to WO2.90 and further to W powder. After compacted with a rubber die, the nanoscale tungsten powder was sintered in a high-tem...Nanoscale tungsten powder was prepared by reducing nanoscale tungsten trioxide in hydrogen to WO2.90 and further to W powder. After compacted with a rubber die, the nanoscale tungsten powder was sintered in a high-temperature dilatometer to investigate its shrinkage process. The results show that the compact of the nanoscale tungsten powder starts to shrink at 1050℃ and ends at 1500℃. The shrinkage rate reaches the maximum value at 1210℃8. The relative density of sintered samples is 96.4%, and its grain size is about 5.8 μm.展开更多
基金This work was financially supported by the National High-Tech Research and Development Program of China (No. 2002AA331090).
文摘Nanoscale tungsten powder was prepared by reducing nanoscale tungsten trioxide in hydrogen to WO2.90 and further to W powder. After compacted with a rubber die, the nanoscale tungsten powder was sintered in a high-temperature dilatometer to investigate its shrinkage process. The results show that the compact of the nanoscale tungsten powder starts to shrink at 1050℃ and ends at 1500℃. The shrinkage rate reaches the maximum value at 1210℃8. The relative density of sintered samples is 96.4%, and its grain size is about 5.8 μm.