FORMATION OF AMORPHOUS Ni-Ti ALLOY BY MECHANICAL ALLOYING 被引量:1
1
作者 Liang Guoxian wang erde Li Zhiming(College of Materials Science and Engineering, Harbin Institute of Technologg,Harbin 150001) 《中国有色金属学会会刊:英文版》 CSCD 1994年第4期83-86,90,共5页
FORMATIONOFAMORPHOUSNi-TiALLOYBYMECHANICALALLOYING¥LiangGuoxian;WangErde;LiZhiming(CollegeofMaterialsScience... FORMATIONOFAMORPHOUSNi-TiALLOYBYMECHANICALALLOYING¥LiangGuoxian;WangErde;LiZhiming(CollegeofMaterialsScienceandEngineering,Ha... 展开更多
关键词 mechanical ALLOYING NI-TI ALLOYS amorphization
下载PDF
Manufacturing a TiAl alloy by high-energy ball milling and subsequent reactive sintering
2
作者 QU Shengguan LI Xiaoqiang +2 位作者 LI Yuanyuan HU Lianxi wang erde 《Rare Metals》 SCIE EI CAS CSCD 2006年第1期21-26,共6页
A TiAl alloy was fabricated by high-energy ball milling and subsequent reactive sintering from the mixed powders of Ti and Al. High-energy ball milling produced a kind of particular composite powders with an extremely... A TiAl alloy was fabricated by high-energy ball milling and subsequent reactive sintering from the mixed powders of Ti and Al. High-energy ball milling produced a kind of particular composite powders with an extremely fine altemative Ti and Al lamella structure. The composite powders not only possessed good consolidation and densification characteristics, but also resulted in the augment of nucleation rate of α and γ titanium aluminides during solid-phase reactive sintering After a series of processing, pressing, degassing, extrusion, and sintering, the resultant TiAl alloy presented high relative density and refined grain sizes of (α2 + γ) lamella and γ phases. The compressive yield strength of the sintered TiAl reached 600 MPa at 800℃. 展开更多
关键词 TiAl alloy high-energy ball milling reactive sintering