Cr掺杂对β-MnO_(2)晶体结构和性能的影响
1
作者 丁欣颖 王鹏成 +2 位作者 刘静怡 温元斌 卿晨 《云南师范大学学报(自然科学版)》 2023年第1期40-44,共5页
利用一步水热法制备出β-MnO_(2)(MO)和5%Cr掺杂的β-MnO_(2)(CMO),Cr掺杂后MO的(110)晶面间距从0.311 nm增大到0.312 nm,有利于其作为水系锌离子电池正极材料时Zn^(2+)在晶体中的脱嵌,显著提高了电池比容量及充放电过程中的循环稳定性.
关键词 水热法 Cr掺杂β-MnO_(2) 晶面间距 水系锌离子电池 正极材料
下载PDF
Study on Diseased Peanut Leaves by Fourier Transform Infrared Spectroscopy
2
作者 Ou Quanhong Zhao Xingxiang +5 位作者 Hao Jianming Zhou Xiangping Liu Gang Li Lun Zhang Li wen yuanbin 《Plant Diseases and Pests》 CAS 2013年第3期1-3,8,共4页
[ Objective] The paper was to study the application d Fourier transform infrared spectroscopy (FTIR technology) in identification of peanut diseases. [Method] By using FFIR technology, combined with the methods of p... [ Objective] The paper was to study the application d Fourier transform infrared spectroscopy (FTIR technology) in identification of peanut diseases. [Method] By using FFIR technology, combined with the methods of principal component analysis and hierarchical cluster analysis, the healthy leaves and three kinds of diseased leaves ( eereospera black spot, cercospora brown spot and web blotch) were identified in the paper. [ Result ] IR spectra of both diseased and healthy samples were similar, but tiny differences in wave-numbers and absorption intensities of peaks were observed in the range of 1 750 -800 cm-1. Significant differences were found in second derivative speclra in the range of 3 600 - 2 800 and 1 750 -650 cm-1 which were selected to perform principle component and hier- archical cluster analysis. Three principal components had the cumulative contribution rate of 94.9% ; the correct rate of principal component analysis for classifica- tion was 100% and the correct rate of hierarchical cluster analysis for identification reached 94.6%. [ Conclusion] Fourier transform infrared spectroscopy has a tmtential to be develoned as a nowerful means for identification of cren diseases. 展开更多
关键词 YI'IR Peanut leaves DISEASE Principal component analysis Hierarchical cluster analysis
下载PDF
氧化铜纳米片阵列的合成及其锂离子电池负极材料的研究
3
作者 温元斌 郭志忠 +9 位作者 卿晨 李天瑞 孙茂欧 杨许月 杨红萍 严泉炜 夏新淼 鲁金宝 段明叶 于素甫江 《激光与光电子学进展》 CSCD 北大核心 2019年第22期160-164,共5页
通过水浴合成方法简易快速地在铜片基底上合成氧化铜纳米片阵列,10min反应时间下合成的氧化铜纳米片阵列具有最高的初始放电比容量(629.1mA·h·g-1)以及良好的循环特性(100次循环后仍保留初始容量的79.6%)。该阵列结构有效地... 通过水浴合成方法简易快速地在铜片基底上合成氧化铜纳米片阵列,10min反应时间下合成的氧化铜纳米片阵列具有最高的初始放电比容量(629.1mA·h·g-1)以及良好的循环特性(100次循环后仍保留初始容量的79.6%)。该阵列结构有效地解决了传统块体氧化铜材料作为锂离子电池负极材料在充电中体积膨胀的问题,同时缩短了锂离子在氧化铜晶格内的扩散距离,提高了氧化铜材料的比容量和氧化铜作为负极材料的性能。 展开更多
关键词 材料 氧化铜 纳米片阵列 锂离子电池